MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aclo Accutech Polypropylene Homopolymer HP0336G15M15CL Glass/Mineral Reinforced Coupled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Glass/Mineral Reinforced

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inMD; ASTM D955
Melt Flow 3.0 g/10 min3.0 g/10 minASTM D1238
Ash 30 %30 %ASTM D2584
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8787ASTM D785
Tensile Strength at Break 49.0 MPa7110 psiASTM D638
Tensile Strength, Yield 51.0 MPa7400 psiASTM D638
Elongation at Break 6.0 %6.0 %ASTM D638
Elongation at Yield 4.0 %4.0 %ASTM D638
Tensile Modulus 3.699 GPa536.5 ksiASTM D638
Flexural Strength 80.0 MPa11600 psiASTM D790
Flexural Modulus 4.599 GPa667.1 ksiASTM D790
Izod Impact, Notched 0.534 J/cm1.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 152 °C306 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 118 °C244 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical IH830A PMMA, General Purpose Grade for Injection Molding
Bamberger Polymers Bapolene® 4072 Polypropylene, Injection Grade
Akro-Plastic Akromid® B3 GF 20 2 RM-D (3375) PA 6 Dry, 20% Glass Fiber Filled
Aclo Accutech Polypropylene Homopolymer HP0336M40L Mica Reinforced
Aclo Accutech Polypropylene Homopolymer HP0336M30CL Mica Reinforced Coupled

PACLO179 / 22434

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.