MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 218G2 V50 Black 34N PA 66 50% Glass Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Description: TECHNYL® A 218G2 V50 Black 34N is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. The product is available in black color.

Key Properties: Excellent glycol resistance; Mechanical performance; Heat stabilized

Benefits: Technyl® A218G2 V50 Black 34N has been specially designed to improve its resistance to automotive cooling liquids, increasing lifetime of parts in permanent contact with such a liquid. Due to high content of glass fibers it offers also an excellent combination between thermal and mechanical properties

Applications: Technyl® A 218G2 V50 Black 34N is used in the automotive industry, for engine parts linked to cooling and heating systems that required a high level of mechanical resistance.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 160 MPa23200 psiISO 527 Type 1A
Elongation at Break 3.5 %3.5 %ISO 527 Type 1A
Tensile Modulus 12.0 GPa1740 ksiISO 527 Type 1A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218G2 V50 Black 34N PA 66 50% Glass Reinforced, Dry
Domo TECHNYL® A 30 H1 V25 PA66, 25% glass fiber, DRY
Domo TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY
Domo TECHNYL® A 218 V40 Black 21 N PA 66 40% Glass Reinforced, Conditioned
Domo TECHNYL® 2412GHF6 PA66, 33% glass fiber, DRY

PSOLVAY839 / 218567

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.