MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ZEON Nipol® DN4555 Nitrile Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nipol® nitrile elastomers are recommended when oil or solvent resistance is needed for the proper functioning of rubber parts. Fuel, oil and solvent resistance improves as acrylonitrile content is increased. Low temperature flexibility and resiliency are improved as butadiene content increases.

High ACN for balance of low temperature, fuel resistance and low fuel permeability

Key Words: NBR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/cc
Mooney Viscosity 48 - 63
@Temperature 100 °C
48 - 63
@Temperature 212 °F
(1+4)
 
Descriptive Properties
AO TypeNS
Hot/ColdC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ChevronTexaco Delo® 100 Motor Oil, SAE 20
ZEON Nipol® DN3650 Nitrile Elastomer
ZEON Zetpol® 2010L Hydrogenated Nitrile Elastomomer
ZEON Zetpol® 2000 Hydrogenated Nitrile Elastomomer
ZEON Hydrin® T3000 Polyepichlorohydrin Elastomer

PZEONB13 / 72972

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.