Armacell Monarch® F-02055 (Black) Neoprene Based Rubber Foam
Categories:
Polymer
;
Thermoset
;
Rubber or Thermoset Elastomer (TSE)
Material Notes:
UL94 HF-1 & HBF listed for flame
Widely used, firm Neoprene based material
ASTM D10569-07 2A5 grade material
12 lb/ft3 density closed cell material
Fine ell-manufactured in blocks (buns)
Information provided by Armacell®
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.160
-
0.224
g/cc
0.00579
-
0.00810
lb/in³
ASTM D1056
Water Absorption
<= 5.0 %
<= 5.0 %
ASTM D1056
Mechanical Properties
Metric
English
Comments
Hardness, Shore OO
65 - 75
65 - 75
ASTM D2240
Tensile Strength
1.03
MPa
150
psi
ASTM D412, Die A
Elongation at Break
125 %
125 %
ASTM D412, Die A
Compressive Strength
0.117
-
0.172
MPa
@Strain 25 %
17.0
-
25.0
psi
@Strain 25 %
ASTM D1056
Resilience
15
15
[%]; ASTM D2632
Tear Strength
>=
6.14
kN/m
>=
35.0
pli
Die C; ASTM D624
Compression Set
<= 25 %
<= 25 %
ASTM D1056
Thermal Properties
Metric
English
Comments
Maximum Service Temperature, Air
65.6
°C
150
°F
Continuous; ASTM D746
93.3
°C
200
°F
Intermittent; ASTM D746
Minimum Service Temperature, Air
-40.0
°C
-40.0
°F
ASTM D746
Flammability, UL94
HB
@Thickness 2.11 mm
HB
@Thickness 0.0830 in
Descriptive Properties
Accelerated Aging
±30%
Change in Compression Deflection, 7 days at 70°C, ASTM D1056
Color
Black
Flammability
FMVSS302
Pass at >1.75 mm
HF-1
Pass at 1.8-2.1 mm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Armacell Monarch® F-05031 (Black) Neoprene, EPDM, SBR Blend Foam
Eurofoam Porocell POR 303/B/CM CR-Neoprene/NBR Foam
Denka Neoprene 671A Polychloroprene
Denka Neoprene GRT M2 Polychloroprene Rubber
Garlock 5260 Neoprene Sheet Rubber
PARMD086 / 186697
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.