MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical SEETEC R3420 Polypropylene, Random Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Features: Seetec R3420 is a polypropylene-ethylene random copolymer designed for the production of cast films. It has a good clarity due to the optimum content of ethylene and offers optimum balance between optical properties and physical strength. It is suitable for the general purpose of coextruded cast film in food packaging or semi retort pouch being required non slip and medium heat seal temperature. SEETEC R3420 meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520 for food contact.

Applications: CPP Film (Non Slip)

CAS No. 9010-79-1

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D1505
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8484ASTM D785
Tensile Strength, Yield 26.5 MPa3840 psi50mm/min; ASTM D638
Film Elongation at Break, MD >= 500 %>= 500 %ASTM D882
Film Elongation at Break, TD >= 500 %>= 500 %ASTM D882
Elongation at Break <= 500 %<= 500 %50mm/min; ASTM D638
Flexural Modulus 0.883 GPa128 ksiASTM D760
Izod Impact, Notched 0.490 J/cm
@Temperature 23.0 °C
0.918 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Film Tensile Strength at Break, MD 440 MPa63800 psiASTM D882
Film Tensile Strength at Break, TD 340 MPa49300 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 - 170 °C266 - 338 °F
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C176 °FASTM D648
Vicat Softening Point 134 °C
@Load 1.00 kg
273 °F
@Load 2.20 lb
ASTM D1525
Flash Point >= 340 °C>= 644 °F
 
Optical PropertiesMetricEnglishComments
Haze 1.3 %1.3 %ASTM D1003
Gloss 135 %135 %45°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Heat Seal Temperature130°C>1 Kgf, LG Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical SEETEC R3400 Polypropylene Random Copolymer
LG Chemical SEETEC R3450 Polypropylene Random Copolymer
Hyosung Topilene C500H PP
LG Chemical SEETEC M1425 Polypropylene Impact Copolymer
LG Chemical SEETEC R1610 Polypropylene Random Copolymer

PLAY386 / 148396

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.