MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elektro-Isola Etronit 201M S Phenolic, Paper Reinforcement, Black, Sheets
Categories: Polymer; Thermoset; Phenolic

Material Notes: Description: Grade with high mechanical properties but the lowest electrical properties of all Etronit types. Used for mechanical applications. The material is black throughout. Used where the mechanical properties are important and where a decorative black laminate is required.

Information provided by Elektro-Isola

Key Words: IEC/EN 60893-3-1 PF CP 201, NEMA LI 1 X
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc
@Temperature 23.0 °C
0.0506 lb/in³
@Temperature 73.4 °F
24h/23°C/50% RH; ISO 1183-A
Water Absorption 2.7 %2.7 %ISO 62-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 130 MPa
@Thickness >=1.50 mm
18900 psi
@Thickness >=0.0591 in
24h/23°C/50% RH; ISO 527
Flexural Strength 170 MPa
@Thickness >=1.50 mm
24700 psi
@Thickness >=0.0591 in
24h/23°C/50% RH, Normal to laminate plane; ISO 178
Flexural Modulus 8.00 GPa
@Thickness >=1.50 mm
1160 ksi
@Thickness >=0.0591 in
24h/23°C/50% RH, Normal to laminate plane; ISO 178
Compressive Strength 310 MPa
@Thickness >=5.00 mm
45000 psi
@Thickness >=0.197 in
24h/23°C/50% RH, , Normal to laminate plane; ISO 604
Shear Strength 35.0 MPa
@Thickness >=5.00 mm
5080 psi
@Thickness >=0.197 in
Parallel, 24h/23°C/50% RH; IEC 60893-2
Izod Impact, Notched (ISO) 3.50 kJ/m²
@Thickness >=5.00 mm
1.67 ft-lb/in²
@Thickness >=0.197 in
Parallel, 24h/23°C/50% RH; ISO 180/2A
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 5.00e+6 ohm5.00e+6 ohmafter immersion in water for 24 hr at 23°C; IEC 60167
Dielectric Strength 0.0394 kV/mm
@Thickness >=3.00 mm,
Temperature 90.0 °C
1.00 kV/in
@Thickness >=0.118 in,
Temperature 194 °F
after 1 hour in oil, Parallel to laminate plane; IEC 60243-1
Comparative Tracking Index 100 V
@Thickness >=3.00 mm
100 V
@Thickness >=0.118 in
24h/23°C/50% RH; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C
@Thickness >=3.00 mm,
Time 7.20e+7 sec
248 °F
@Thickness >=0.118 in,
Time 20000 hour
IEC 60216
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hippe PF CP 201 Cellulose Paper Reinforced Phenolic Resin - Sheet
Elektro-Isola Etronit 201M Phenolic, Paper Reinforcement, Dark Brown, Sheets
Norplex-Micarta NP611R Phenolic Paper Laminate Sheet, NEMA XP
Aclo Accutech ABS ABS831G10L Glass Reinforced

PELEKT025 / 126901

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.