MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 Dexron® -VI ATF
Categories: Fluid; Lubricant

Material Notes: DEXRON®-VI ATF is a synthetic transmission fluid approved for use in passenger car and light truck automatic transmissions that require a GM DEXRON® -VI or earlier generation DEXRON® fluid. It is particularly recommended for use in new GM 6-speed automatic transmissions, and is fully backward compatible for use in older GM automatic transmissions. DEXRON®-VI ATF is specifically engineered to help ensure long service life, provide better performance under extreme operating conditions, and provide consistent shift performance for the life of the fluid. It provides significantly improved oxidation stability, shear stability, friction durability and foam resistance compared with DEXRON®-III H fluids, as well as improved low-temperature performance.

Applications:

  • Service fill in all automatic transmissions that require a GM DEXRON®-VI or earlier-generation DEXRON® transmission fluid
  • Hydraulic systems on industrial and mobile equipment operating over a wide temperature range
DEXRON®-VI ATF is approved for service fill where the OEM specifies:
  • GM DEXRON®-VI (License No. J-60004)
DEXRON®-VI ATF meets or exceeds the requirements of:
  • Denison Hydraulics HF-0
  • Vickers (Eaton) M-2950-S, I-286-S
Features/Benefit:
  • Meets stricter performance requirements for new GM 6-speed automatic transmissions
  • Outstanding friction durability for consistent shift performance for the life of the fluid
  • Excellent oxidation resistance and thermal stability for long fluid life
  • Protects against sludge and varnish formation
  • Protects against wear
  • Protects against rust and corrosion
  • High shear stability
  • Excellent low-temperature properties
  • Good seal compatibility
  • Good foam resistance
  • Backward compatible for use in older GM automatic transmissions

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.847 g/cc0.847 g/cc
Density 0.845 g/cc0.0305 lb/in³
Brookfield Viscosity 11500 cP
@Temperature -40.0 °C
11500 cP
@Temperature -40.0 °F
Viscosity Measurement 153153Index
Kinematic Viscosity at 40°C (104°F) 29.8 cSt29.8 cSt
Kinematic Viscosity at 100°C (212°F) 6.0 cSt6.0 cSt
 
Thermal PropertiesMetricEnglishComments
Pour Point <= -45.0 °C<= -49.0 °F
Flash Point 229 °C444 °FCOC
 
Component Elements PropertiesMetricEnglishComments
Zinc, Zn <= 0.0020 %<= 0.0020 %
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubriplate DEXRON III / MERCON Automatic Transmission Fluid Motor Oil & Transmission Fluid
Phillips 66 Kendall® DEXRON®-VI ATF
ChevronTexaco Havoline® MERCON®/DEXRON®-III Automatic Transmission Fluid
ChevronTexaco DEXRON®-III/MERCON® Automatic Transmission Fluid

WCON6026 / 210141

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.