MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Murtfeldt Murytal® H Acetal Homopolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes: In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.

Special Properties:
• High rigidity
• Excellent ability to regain its form
• Extremely good electric isolation properties
• Practically no moisture absorption
• Good resistance to chemicals (pH 4 – 9)
• Approved for use in the food industry (EU and FDA)
• Extremely good machinability

Information provided by Murtfeldt Kunststoffe GmbH & Co. KG.

Key Words: POM-H
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³ISO 1183-1
Moisture Absorption at Equilibrium 0.20 %
@Temperature 23.0 °C
0.20 %
@Temperature 73.4 °F
50% RH
Water Absorption at Saturation 0.80 %
@Temperature 23.0 °C
0.80 %
@Temperature 73.4 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8888dry; ISO 2039-2
Hardness, Shore D 8383DIN 53505
Ball Indentation Hardness 160 MPa23200 psidry; ISO 2039-1
Tensile Strength, Yield 78.0 MPa11300 psidry; ISO 527-1
 78.0 MPa11300 psi50% RH; ISO 527-1
Elongation at Break 50 %50 %dry; ISO 527-1
 50 %50 %50% RH; ISO 527-1
Creep Strength  15.0 MPa
@Time 3.60e+6 sec
2180 psi
@Time 1000 hour
stress leading to 1% elongation; dry; ISO 899-1
 15.0 MPa
@Time 3.60e+6 sec
2180 psi
@Time 1000 hour
stress leading to 1% elongation; 50% RH; ISO 899-1
Modulus of Elasticity 3.30 GPa479 ksidry
 3.30 GPa479 ksi50% RH
Compressive Yield Strength  22.0 MPa
@Strain 1 %
3190 psi
@Strain 1 %
dry; ISO 604
 40.0 MPa
@Strain 2 %
5800 psi
@Strain 2 %
dry; ISO 604
 75.0 MPa
@Strain 5.0 %
10900 psi
@Strain 5.0 %
dry; ISO 604
Charpy Impact Unnotched 20.0 J/cm²95.2 ft-lb/in²dry; ISO 179-1/1eU
 >= 20.0 J/cm²>= 95.2 ft-lb/in²ISO 179
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²dry; ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.340.34
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmdry; IEC 60093
 >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm50% RH; IEC 60093
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmdry; IEC 60093
 >= 1.00e+13 ohm>= 1.00e+13 ohm50% RH; IEC 60093
Dielectric Constant  3.8
@Frequency 100 Hz
3.8
@Frequency 100 Hz
dry; IEC 60250
 3.8
@Frequency 100 Hz
3.8
@Frequency 100 Hz
50% RH; IEC 60250
 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
dry; IEC 60250
 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
50% RH; IEC 60250
Dielectric Strength 20.0 kV/mm508 kV/indry; IEC 60243-1
 20.0 kV/mm508 kV/in50% RH; IEC 60243-1
Dielectric Loss Index  0.0030
@Frequency 100 Hz
0.0030
@Frequency 100 Hz
dry; IEC 60250
 0.0030
@Frequency 100 Hz
0.0030
@Frequency 100 Hz
50% RH; IEC 60250
 0.0080
@Frequency 1e+6 Hz
0.0080
@Frequency 1e+6 Hz
dry; IEC 60250
 0.0080
@Frequency 1e+6 Hz
0.0080
@Frequency 1e+6 Hz
50% RH; IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear  95.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
52.8 µin/in-°F
@Temperature 73.4 - 140 °F
 110 µm/m-°C
@Temperature 23.0 - 100 °C
61.1 µin/in-°F
@Temperature 73.4 - 212 °F
Thermal Conductivity 0.310 W/m-K2.15 BTU-in/hr-ft²-°F
Melting Point 180 °C356 °FISO 11357-1
Maximum Service Temperature, Air  90.0 °C
@Time 7.20e+7 sec
194 °F
@Time 20000 hour
 105 °C
@Time 1.80e+7 sec
221 °F
@Time 5000 hour
 150 °C
@Time <=86400 sec
302 °F
@Time <=24.0 hour
Minimum Service Temperature, Air -50.0 °C-58.0 °F
Glass Transition Temp, Tg -50.0 °C-58.0 °FISO 11357-1
Flammability, UL94 HBHB
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
ColorNatural/Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Stat-Tech™ AT-CB2/000 CR Acetal (POM) Copolymer
Röchling SUSTARIN® H AF - DE588 POM/Acetal Homopolymer
Ensinger Tecaform™ UD Blue Ultra Detectable Acetal Copolymer (POM)
Ensinger Tecaform™ MT Acetal, Medical Grade (POM)
DuPont Mobility and Materials Delrin® FG570 NC000 Acetal Homopolymer

PMURT928 / 156575

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.