MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Momentive Performance Materials XE23-B2484 Heat Cured Rubber - Electro Conductive
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance standards.

XE23-B2484 is a specialty grade, peroxide curable silicone elastomer.

Key Feature: Vol. Res. 2 Ohm/cm

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7575
Tensile Strength 7.20 MPa1040 psi
Elongation at Break 180 %180 %
Tear Strength 20.0 kN/m114 pliangle
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.0 ohm-cm2.0 ohm-cm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials TSE 221-7U Heat Cured Rubber
Parker Chomerics Tecknit SC-Consil® 862 Carbon-Filled Silicone Elastomer
NuSil R-1550 Silicone, Electrically Conductive
Momentive Performance Materials Silopren™ LSR 2345/05 Electrically-Conductive Liquid Silicone Rubber
Momentive Performance Materials Silopren™ LSR 2345/04 Electrically-Conductive Liquid Silicone Rubber

PGE8V865 / 109125

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.