MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding. This product is available in Natural & Black.

Key Properties: UL94 V0 at 0.8mm and Excellent filling qualities

Benefits: This Red Phosphorous flame retardent grade provides robust UL 94 V-0 and a full UL yellow card while offering good mechanical properties. This grade is suitable for moulding insulating parts for electrical devices, and more generally for thin parts under stress.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/E.C.This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications

Applications: Industrial controls and electrical insulation system

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³ISO 1183/A
Water Absorption 0.75 %
@Temperature 23.0 °C,
Time 86400 sec
0.75 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Viscosity  110 cP
@Shear Rate 1000 1/s,
Temperature 300 °C
110 cP
@Shear Rate 1000 1/s,
Temperature 572 °F
 200 cP
@Shear Rate 1000 1/s,
Temperature 280 °C
200 cP
@Shear Rate 1000 1/s,
Temperature 536 °F
 200 cP
@Shear Rate 100 1/s,
Temperature 300 °C
200 cP
@Shear Rate 100 1/s,
Temperature 572 °F
 300 cP
@Shear Rate 100 1/s,
Temperature 280 °C
300 cP
@Shear Rate 100 1/s,
Temperature 536 °F
Linear Mold Shrinkage 0.0055 cm/cm0.0055 in/inIsotropy
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/in
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 140 MPa20300 psiISO 527 Type 1A
Tensile Stress at Strain  30.0 MPa
@Strain 0.5 %
4350 psi
@Strain 0.5 %
 95.0 MPa
@Strain 1 %
13800 psi
@Strain 1 %
 130 MPa
@Strain 1.5 %
18900 psi
@Strain 1.5 %
 150 MPa
@Strain 2 %
21800 psi
@Strain 2 %
 170 MPa
@Strain 2.5 %
24700 psi
@Strain 2.5 %
Elongation at Break 2.0 %2.0 %ISO 527 Type 1A
Tensile Modulus 9.00 GPa1310 ksiISO 527 Type 1A
Flexural Strength 250 MPa36300 psiISO 178
Flexural Modulus 7.50 GPa1090 ksiISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant 3.43.4IEC 60250
Dielectric Strength 25.0 kV/mm635 kV/inIEC 60243
Dissipation Factor 0.0200.020IEC 60250
Comparative Tracking Index 250 V250 VSolution B; IEC 60112
 300 V300 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.1 µm/m-°C
@Temperature 23.0 - 85.0 °C
16.7 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 263 °C505 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FISO 75/Af
Flammability, UL94  V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
ISO 1210
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
ISO 1210
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
ISO 1210
Oxygen Index 30.5 %30.5 %ISO 4589
Glow Wire Ignition Temperature 725 °C1340 °FISO 60695-2-13
Glow Wire Flammability Index 960 °C1760 °FISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 270 - 275 °C518 - 527 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone275-280°C
Fire and smoke F indexI3/F3NF F 16 101
Mixing Zone280-285°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo Technyl® C216V30 30% Glass Filled Nylon 6
Domo TECHNYL® A 20 V25 PA66, 25% glass fiber, Conditioned
Domo TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY
Domo TECHNYL® C 216 V30 PA6, 30% glass fiber, DRY
Domo TECHNYL® 2411GF6 PA66, 30% glass fiber, DRY

PRHOD584 / 137815

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.