MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Petroquimica Triunfo Trithene® SX 7012 LDPE - Blow Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: The Trithene SX 7012 resin is a low density polyethylene (LDPE) with medium molecular weight which allows the production of flasks with an adequate combination of mechanical and impact strength, flexibility, and good stress cracking resistance -ESCR. Its easy processability also allows high moulding productivity, thickness control, and excellent surface appearance. There are no other components or additives included in this product formulation. Therefore there is no restriction for this product to be in contact with medical or pharmaceutical goods and other products that demand high packing purity. This product complies with ASTM standard D1248-IA3 and the requirements of The United States Pharmacopeia - Phisico-Chemical Tests Plastics, to contact with pharmaceutical goods.

Applications: Flexible flasks for medical and pharmaceutical goods, small and medium size semi-stiff and transparent containers requiring no sterilization. Depending on processing condition, can be sterilized at temperatures lower than 110 ºC.

Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C.

Information provided by Dax Resinas

Petroquimica Triunfo has been acquired by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 - 0.923 g/cc0.0333 - 0.0333 lb/in³ASTM D1505
Melt Index of Compound 1.0 - 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 - 4.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9393ASTM D2240
Tensile Strength at Break 12.0 MPa1740 psiASTM D638
Tensile Strength, Yield 10.0 MPa1450 psiASTM D638
Elongation at Break 490 %490 %ASTM D638
Secant Modulus 0.128 GPa18.6 ksi5%; ASTM-D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 111 °C232 °FASTM D3418
Vicat Softening Point 91.0 °C196 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Melt Temperature 165 - 175 °C329 - 347 °F
Mold Temperature 15.0 - 15.0 °C59.0 - 59.0 °F(close to)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Petroquimica Triunfo Trithene® SX 7010 LDPE - Blow Molding
Braskem PB682 Blow Molding Low Density Polyethylene
Braskem PB 601 LDPE Blow Molding Polyethylene
Braskem PB 526 LDPE Blow Molding Polyethylene
Braskem Green PE SLL5405S Blown Film Extrusion High Density Polyethylene

PDAX100 / 29525

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.