MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Kelon® B FR H CETG/250-V0 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.56 g/cc0.0564 lb/in³
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/in
Linear Mold Shrinkage, Transverse 0.0040 - 0.0065 cm/cm0.0040 - 0.0065 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  35.0 MPa
@Temperature 150 °C
5080 psi
@Temperature 302 °F
 50.0 MPa
@Temperature 120 °C
7250 psi
@Temperature 248 °F
 60.0 MPa
@Temperature 90.0 °C
8700 psi
@Temperature 194 °F
 75.0 MPa
@Temperature 60.0 °C
10900 psi
@Temperature 140 °F
 90.0 MPa
@Temperature 23.0 °C
13100 psi
@Temperature 73.4 °F
Elongation at Break  2.0 %
@Temperature 23.0 °C
2.0 %
@Temperature 73.4 °F
 2.5 %
@Temperature 60.0 °C
2.5 %
@Temperature 140 °F
 6.2 %
@Temperature 90.0 °C
6.2 %
@Temperature 194 °F
 10 %
@Temperature 120 °C
10 %
@Temperature 248 °F
 15 %
@Temperature 150 °C
15 %
@Temperature 302 °F
Tensile Modulus  2.60 GPa
@Temperature 150 °C
377 ksi
@Temperature 302 °F
 3.50 GPa
@Temperature 120 °C
508 ksi
@Temperature 248 °F
 4.50 GPa
@Temperature 90.0 °C
653 ksi
@Temperature 194 °F
 7.20 GPa
@Temperature 60.0 °C
1040 ksi
@Temperature 140 °F
 10.0 GPa
@Temperature 23.0 °C
1450 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched  2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
 2.50 J/cm²
@Temperature -20.0 °C
11.9 ft-lb/in²
@Temperature -4.00 °F
Charpy Impact, Notched  0.400 J/cm²
@Temperature -20.0 °C
1.90 ft-lb/in²
@Temperature -4.00 °F
 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 500 V500 VA solution
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 115 °C239 °F
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °F
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °F
Vicat Softening Point 190 °C
@Load 5.00 kg
374 °F
@Load 11.0 lb
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
Oxygen Index 32 %32 %
Glow Wire Test  960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
GWFI/GWT
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
GWFI/GWT
Glow Wire Ignition Temperature  800 °C
@Thickness 2.00 mm
1470 °F
@Thickness 0.0787 in
 825 °C
@Thickness 1.00 mm
1520 °F
@Thickness 0.0394 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 260 °C464 - 500 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 90.0 - 100 °C
@Time 10800 sec
194 - 212 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Domo Technyl® C 218 MT25 V15 25% Mineral, 15% Glass Filled, Heat Stabilized Nylon 6
Envalior Akulon® K224-LGM35 PA6-(GF+MD)40, Dry, 15/25% Glass/Mineral Filled
Envalior Akulon® Ultraflow K-FHGM35 PA6-(GF+MD)40, Dry, 15/25% Glass/Mineral Filled, Heat Stabilized
LATI Kelon® B H CETG/300 PA 6, Glass/Mineral Reinforced, Heat Stabilized

PLATH9606 / 177302

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.