MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meehanite HR Heat Resisting Cast Iron
Categories: Metal; Ferrous Metal; Cast Iron

Material Notes: Type HR is a strong, dense iron of high rigidity and excellent resistance to scaling under most conditions. It possesses good load carrying ability. Recommended for service conditions without thermal shock such as furnace parts, retorts, tube support, etc.

General Meehanite information - Meehanite metal is first melted to a definite degree of undercooling or constitution which is related to the section of the casting to be poured and the range of physical properties such as tensile strength and hardness required. Nucleation with patented mixtures of graphitizing agents results in the removal of undercooling, in the controlled precipitation of graphite and in a fine grained eutectic cell structure which determines the density and physical integrity of the casting. Ordinary cast irons made to chemical specifications which do not include the benefit of controlled undercooling are influenced by mass effect to a maximum degree and for this and other reasons cannot be considered an equivalent to Meehanite metal.

Information provided by Meehanite Marketing Association.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell >= 300>= 300Nominal
Tensile Strength, Ultimate 276 MPa40000 psi
Modulus of Elasticity 145 GPa21000 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.4 µm/m-°C
@Temperature 37.8 - 538 °C
7.43 µin/in-°F
@Temperature 100 - 1000 °F
Thermal Conductivity 51.9 W/m-K
@Temperature 10.0 - 232 °C
360 BTU-in/hr-ft²-°F
@Temperature 50.0 - 450 °F
Maximum Service Temperature, Air 732 °C1350 °Fnongrowing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Meehanite HS Heat Resisting Cast Iron
Meehanite GE-30 Flake Graphite Cast Iron
Meehanite Ductliron® SH-100 Nodular Graphite Ductile Iron

NMEE20 / 18241

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.