MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos H03G-01 Polypropylene Homopolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: This is a homopolymer designed for tenter frame BOPP processing and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.

    Applications
  • Food packaging
  • Overwrap
  • Metallized film

    Benefits
  • Barefoot
  • Good optical properties
  • High strength properties

Information provided by Ineos Olefins & Polymers USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.904 - 0.908 g/cc0.0327 - 0.0328 lb/in³ASTM D1505
Linear Mold Shrinkage 0.010 - 0.025 cm/cm0.010 - 0.025 in/inASTM D955
Melt Flow 3.4 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.4 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 79 - 10879 - 108ASTM D785
Tensile Strength, Yield 31.6 MPa
@Temperature 23.0 °C
4580 psi
@Temperature 73.4 °F
Molded and tested under D410, 50 mm/min; ASTM D638
Elongation at Yield 10 %10 %50 mm/min; ASTM D638
Flexural Modulus 1.30 GPa
@Temperature 23.0 °C
188 ksi
@Temperature 73.4 °F
ASTM D790A
Izod Impact, Notched 0.214 - 0.374 J/cm
@Temperature 23.0 °C
0.400 - 0.700 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C189 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos H02C-00 Polypropylene Homopolymer
Ineos H03G-05 Polypropylene Homopolymer
Ineos H05A-00 Polypropylene Homopolymer
Ineos H08U-00 Polypropylene Homopolymer, Fiber Grade
Ineos H12G-00 Polypropylene Homopolymer

PINEOS023 / 99344

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.