MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

BASF Ultrason® E 2010 MR HP PESU
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: Description: Unreinforced, medium viscosity standard injection molding grade for improved demolding behavior with Mold Release. PES-Blend with improved processibility. (High Productivity) Abbreviated designation according to ISO 1043-1: PESU.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.700 - 0.800 g/cc0.0253 - 0.0289 lb/in³
Density 1.33 g/cc0.0480 lb/in³ISO 1183
Water Absorption 1.7 %1.7 %ISO 62
Moisture Absorption at Equilibrium 0.50 %0.50 %23°C; 50% RH; ISO 62
Viscosity Test 56 cm³/g0.56 dl/gISO 307
Linear Mold Shrinkage, Flow 0.0076 cm/cm0.0076 in/inISO 2577, 294-4
Linear Mold Shrinkage, Transverse 0.0085 cm/cm0.0085 in/inISO 2577, 294-4
Melt Flow 93.1 g/10 min
@Load 10.0 kg,
Temperature 360 °C
93.1 g/10 min
@Load 22.0 lb,
Temperature 680 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 192 MPa27800 psiISO 2039-1
Tensile Strength, Yield 85.0 MPa12300 psi50mm/min; ISO 527-1/-2
Elongation at Break 80 %80 %Nominal; ISO 527-1/-2
Elongation at Yield 6.4 %6.4 %50mm/min; ISO 527-1/-2
Tensile Modulus 2.70 GPa392 ksiISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 220 °C428 °F
Decomposition Temperature >= 400 °C>= 752 °F
Ignition Temperature 580 - 600 °C1080 - 1110 °FDIN 54836
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FHopper throat
Zone 1 340 °C644 °FFeed zone
Zone 2 350 °C662 °FCompression
Zone 3 360 °C680 °FMetering-zone
Zone 4 360 °C680 °FNozzle
Melt Temperature 360 °C680 °FOptimal
 340 - 390 °C644 - 734 °FInjection molding/extrusion
Mold Temperature 140 - 180 °C284 - 356 °FInjection molding
 160 °C320 °FOptimal
Drying Temperature 140 °C284 °F
Dry Time 4 hour4 hour
 
Descriptive Properties
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultrason® E 2010 HC PESU
BASF Ultrason® E 2010 SW Q31 10088 PESU
BASF Ultrason® E 2020 P SR PESU
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE
Overview of materials for Nylon 66/6

PBASG0176 / 131809

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.