MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aurora Plastics TufGuard M™ GPP1001VOM-HCO PP, Flame Retardant
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: Application: UL-94 V0 Flame Retardant/Impact Resistant Polypropylene

Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 - 1.02 g/cc0.980 - 1.02 g/ccASTM D792
Melt Flow 13 - 17 g/10 min13 - 17 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 22.8 MPa>= 3300 psiASTM D638
Elongation at Break >= 60 %>= 60 %ASTM D638
Flexural Modulus 1.21 GPa175 ksitangent; ASTM D790
Izod Impact, Notched >= 1.60 J/cm>= 3.00 ft-lb/inASTM D256
Dart Drop Total Energy >= 8.01 J/cm>= 0.0150 ft-lb/milASTM D5420
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
Oxygen Index >= 28 %>= 28 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aurora Plastics TufGuard M™ GPP1001VOM-HCO-15 PP, Flame Retardant
Avient Maxxam™ FR PP FR 8-6 A NATURAL - ROHS Polypropylene
RTP Company RTP 150 HI UV Polypropylene (PP), High Impact - Flame Retardant - UV Stabilized
RTP Company RTP 156 Polypropylene (PP), Copolymer - Flame Retardant - UL94 V-0
RTP Company RTP 199 X 138320 B Polypropylene (PP); Flame Retardant - UV Stabilized

PSEPN122 / 179126

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.