MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Nordel® IP 4725P Medium Hardness Dense Extrusion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nordel® IP 4725P is a low viscosity semicrystalline grade which offers ease of processing, fast cure rates and high states of cure with standard sulfur cure systems. It is designed for molded and extruded applications requiring low viscosity, high green strength and high finished hardness. It is ideally suited for high hardness extruded profiles and molded goods. It can also be peroxide cured.

Information provided by manufacturer.

Key Words: 0640-03-08
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.362 g/cc0.04921 lb/in³
Mooney Viscosity 70
@Temperature 100 °C
70
@Temperature 212 °F
ML 1 + 4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8282Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 11.1 MPa1610 psiVulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 393 %393 %Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 4.50 MPa
@Strain 100 %
653 psi
@Strain 100 %
Vulcanizate, Press cured, TC95 +3min at 160°C
200% Modulus 6.90 MPa
@Strain 200 %
1000 psi
@Strain 200 %
Vulcanizate, Press cured, TC95 +3min at 160°C
300% Modulus 9.10 MPa
@Strain 300 %
1320 psi
@Strain 300 %
Vulcanizate, Press cured, TC95 +3min at 160°C
Tear Strength 30.7 kN/m175 pliDie C, Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 93 %
@Temperature 125 °C
93 %
@Temperature 257 °F
Pellets cured MDR TC95 + 15 min at 160°C, 70 hr at 125°C; Method B
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -25.0 °C-13.0 °FTemperature Retraction, TR-10
 
Descriptive Properties
Formulation as Tested0.5ZnDBC
 0.7TMTD
 0.8DPTH
 1.5MBTS
 1.5Sulfur
 10Paraffinic Oil
 100Nordel® IP 4725P
 2Stearic Acid
 5Zinc Oxide
 60N-550 Black
 8Calcium Oxide
 80Precipitated Calcium Carbonate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Nordel® IP 4725P General Purpose Molding
Dow Nordel® IP 4725P Heat Resistant Molding
Dow Nordel® IP 4725P High Hardness Extruded Profile
Dow Nordel® IP 4520 Molded Golf Grip
Dow Nordel® IP 5565 General Purpose Molding

PDVG25 / 34145

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.