MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Azoty Tarnow™ TARNOFORM 300 GF6 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 30% Glass Fiber Reinforced

Material Notes: 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.

Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.63 g/cc0.0589 lb/in³ISO 1183
Water Absorption 0.50 %0.50 %ISO 62
Linear Mold Shrinkage 0.0102 cm/cm
@Thickness 4.00 mm
0.0102 in/in
@Thickness 0.157 in
Melt Flow 4.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.3 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 200 MPa29000 psi358 N; ISO 2039-1
Tensile Strength at Break 120 MPa17400 psiISO 527
Elongation at Break 3.5 %3.5 %ISO 527
Tensile Modulus 9.30 GPa1350 ksiISO 527
Flexural Strength 176 MPa25500 psiISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²1A; ISO 180
Charpy Impact, Notched 0.570 J/cm²2.71 ft-lb/in²1eA; ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant  4.2
@Frequency 100 Hz
4.2
@Frequency 100 Hz
IEC 60250
 4.2
@Frequency 1e+6 Hz
4.2
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 30.0 kV/mm762 kV/inIEC 60243
Dissipation Factor 0.0095
@Frequency 1e+6 Hz
0.0095
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.21 J/g-°C0.289 BTU/lb-°F
Melting Point 167 °C333 °F10°C/min.; ISO 3146
Maximum Service Temperature, Air 110 °C230 °F
Deflection Temperature at 1.8 MPa (264 psi) 163 °C325 °FISO 75
Vicat Softening Point 162 °C324 °F50 N; ISO 306
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 230 °C356 - 446 °FBarrel temperature
Mold Temperature 60.0 - 120 °C140 - 248 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUCEL GC225 POM+GF25%, High Rigidity
Mitsubishi Iupilon® S3000UR 16.5 MFI, UV Stabilized Polycarbonate With Release
Covestro Apec® HT KU 1-9363 High-Heat Polycarbonate, UV-Stabilized
Covestro Apec® HT KU 1-9353 High-Heat Polycarbonate, UV-Stabilized
Covestro Apec® HT KU 1-9343 High-Heat Polycarbonate, UV-Stabilized

PZAK015 / 72854

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.