MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions Vinyl Rigid Molding MR840 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.34 g/cc1.34 g/ccASTM D792
Melt Flow 16 g/10 min
@Load 21.6 kg,
Temperature 190 °C
16 g/10 min
@Load 47.6 lb,
Temperature 374 °F
Procedure A; ASTM D1238
Spiral Flow 73.7 cm29.0 in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 39.3 MPa5700 psiType I, 51 mm/min; ASTM D638
Elongation at Break 160 %160 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 2.34 GPa339 ksiType I, 5.1 mm/min; ASTM D638
Izod Impact, Notched  1.60 J/cm
@Thickness 3.18 mm,
Temperature -18.0 °C
3.00 ft-lb/in
@Thickness 0.125 in,
Temperature -0.400 °F
Injection Molded; ASTM D256A
 7.50 J/cm
@Thickness 3.18 mm,
Temperature 0.000 °C
14.1 ft-lb/in
@Thickness 0.125 in,
Temperature 32.0 °F
Injection Molded; ASTM D256A
 9.10 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
17.0 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 68.3 °C
@Thickness 3.18 mm
155 °F
@Thickness 0.125 in
Annealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
ALL; UL 94
 
Descriptive Properties
FeaturesGeneral Purpose
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Recycled ContentYes
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Interior Parts
 General Purpose

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fainplast Compounds MGS 75 Medical Flexible PVC, Injection Molding
Teknor Apex Sinvicomp SRF 9702/C Polyvinyl Chloride, Rigid
Fainplast Compounds MRT 168 Medical Rigid PVC, Injection Molding
Fainplast Compounds MRK 267 Medical Rigid PVC, Injection Molding
Crystex Composites Mykroy/Mycalex MM 451 Molding Grade Glass-bonded Mica Composite

PH0POL0573 / 145142

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.