MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexWeb® CR III 1/16-5056-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb  (discontinued **)
Categories: Metal; Metal Foam, Mesh, or Honeycomb; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: Grade is designated as "Cell Size-Alloy-Foil Gauge."
5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb® CR III coating has been developed to offer superior protection for aluminum honeycomb exposed to corrosive environments. The HexWeb® CR III system offers a clear protective film that interacts with the aluminum surface forming a stable, tightly adherent bond. The coating is primarily in an organo-metallic polymer type that differs from the normal conversion-type corrosion protective coatings.
Hexcel expanded honeycomb is manufactured by bonding together sheets of aluminum foil, then expanding to form a cellular honeycomb configuration. Resulting panels have sharp, clean cell walls, are essentially burr-free, and are suitable for high-quality core-to-facing bond.

Aluminum HexWeb® CR III Specification Grade honeycomb materials are predominantly used in sandwich structures to meet design requirements for highly engineered structural components. As a structural core material it finds applications in all types of aerospace vehicles and supporting equipment where sandwich structure offers rigid panels of minimum weight, aerodynamic smooth surfaces, and high fatigue resistance. The same structural properties are also used for commercial applications such as tools, snow and water skis, bulkheads, and floors. Other nonstructural uses are direction air/fluid flow control, RF shielding, and energy absorption.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.147 g/cc0.00532 lb/in³Nominal
 
Mechanical PropertiesMetricEnglishComments
Compressive Yield Strength >= 8.96 MPa>= 1300 psiBare, min, preliminary
 >= 9.65 MPa>= 1400 psiStabilized, min, preliminary
 11.7 MPa1700 psiBare, typical, preliminary
 12.4 MPa1800 psiStabilized, typical, preliminary
Compressive Modulus 3.45 GPa500 ksiStabilized, typical, preliminary
Shear Modulus 0.345 GPa50.0 ksiPlate Shear, W Direction, typical, preliminary
 0.758 GPa110 ksiPlate Shear, L Direction, typical, preliminary
Shear Strength >= 3.17 MPa>= 460 psiPlate Shear, W Direction, min, preliminary
 4.14 MPa600 psiPlate Shear, W Direction, typical, preliminary
 >= 5.24 MPa>= 760 psiPlate Shear, L Direction, min, preliminary
 6.76 MPa980 psiPlate Shear, L Direction, typical, preliminary

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexWeb® CR III 1/8-5056-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Hexcel® HexWeb® CR III 3/8-5052-.005 Corrosion Resistant Specification Grade Aluminum Honeycomb
Hexcel® HexWeb® CR III 1/8-5056-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Hexcel® HexWeb® CR III 1/8-5056-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb
Hexcel® HexWeb® CR III 1/8-5056-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb

PHEXC247 / 98718

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.