MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 5456-H24
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A95456; ISO AlMg5Mn1; Aluminium 5456-H24; AA5456-H24; Al5456-H24
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.66 g/cc0.0961 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 9090500 kg load with 10 mm ball.
Hardness, Knoop 114114Converted from Brinell Hardness Value
Hardness, Rockwell A 38.238.2Converted from Brinell Hardness Value
Hardness, Rockwell B 5656Converted from Brinell Hardness Value
Hardness, Vickers 101101Converted from Brinell Hardness Value
Tensile Strength, Ultimate 370 MPa53700 psi
Tensile Strength, Yield 280 MPa40600 psi
Elongation at Break 13 %13 %In 5 cm
Tensile Modulus 70.3 GPa10200 ksi
Compressive Modulus 71.7 GPa10400 ksi
Notched Tensile Strength 290 MPa42100 psi2.5 cm width x 0.16 cm thick side-notched specimen, Kt = 17.
Ultimate Bearing Strength 669 MPa97000 psiEdge distance/pin diameter = 2.0
Bearing Yield Strength 427 MPa61900 psiEdge distance/pin diameter = 2.0
Poissons Ratio 0.330.33Estimated from trends in similar Al alloys.
Shear Modulus 26.0 GPa3770 ksiEstimated from similar Al alloys.
Shear Strength 210 MPa30500 psiCalculated value.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000590 ohm-cm0.00000590 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  22.1 µm/m-°C
@Temperature -50.0 - 20.0 °C
12.3 µin/in-°F
@Temperature -58.0 - 68.0 °F
 23.9 µm/m-°C
@Temperature 20.0 - 100 °C
13.3 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical; average over range
 24.8 µm/m-°C
@Temperature 20.0 - 200 °C
13.8 µin/in-°F
@Temperature 68.0 - 392 °F
 25.9 µm/m-°C
@Temperature 20.0 - 300 °C
14.4 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.900 J/g-°C0.215 BTU/lb-°F
Thermal Conductivity 116 W/m-K805 BTU-in/hr-ft²-°F
Melting Point 568.3 - 638 °C1055 - 1180 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness
Solidus 568.3 °C1055 °FAA; Typical
Liquidus 638 °C1180 °FAA; Typical
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 343 °C650 °Fholding at temperature not required
Hot-Working Temperature 260 - 510 °C500 - 950 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 91.9 - 94.8 %91.9 - 94.8 %As remainder
Chromium, Cr 0.05 - 0.20 %0.05 - 0.20 %
Copper, Cu <= 0.10 %<= 0.10 %
Iron, Fe <= 0.40 %<= 0.40 %
Magnesium, Mg 4.7 - 5.5 %4.7 - 5.5 %
Manganese, Mn 0.50 - 1.0 %0.50 - 1.0 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.25 %<= 0.25 %
Titanium, Ti <= 0.20 %<= 0.20 %
Zinc, Zn <= 0.25 %<= 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 5456-O
Aluminum 5456-H111
Aluminum 5456-H112
Aluminum 5456-H116; 5456-H321
Aluminum 5456-H25

MA5456H24 / 9286

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.