MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company PermaStat® 300 Polycarbonate (PC), ESD Protection - Permanently Anti-static - UL94 HB
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D 792
Linear Mold Shrinkage 0.0060 - 0.0090 cm/cm
@Thickness 3.17 mm
0.0060 - 0.0090 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 44.8 MPa6500 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Tensile Modulus 1.65 GPa240 ksiASTM D 638
Flexural Strength 62.1 MPa9000 psiASTM D 790
Flexural Modulus 1.79 GPa260 ksiASTM D 790
Izod Impact, Notched 6.41 J/cm
@Thickness 3.17 mm
12.0 ft-lb/in
@Thickness 0.125 in
D 256
Izod Impact, Unnotched NB
@Thickness 3.17 mm
NB
@Thickness 0.125 in
ASTM D4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+8 - 1.00e+11 ohm-cm1.00e+8 - 1.00e+11 ohm-cmASTM D 257
Surface Resistivity per Square 1.00e+10 - 1.00e+12 ohm1.00e+10 - 1.00e+12 ohmASTM D 257
Static Decay <= 2.0 sec<= 2.0 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 104 °C220 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 221 - 243 °C430 - 470 °F
Mold Temperature 65.6 - 121 °C150 - 250 °F
Drying Temperature 121 °C250 °F
Dry Time 4 hour4 hour
Moisture Content 0.020 %0.020 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 41.4 - 68.9 MPa6000 - 10000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company PermaStat® 1800 Nat/Clear Acrylic (PMMA) Permanently Anti-static - ESD Protection - Transparent Grade
RTP Company PermaStat® 1800 MD Acrylic (PMMA); Permanently Anti-static - ESD Protection - Transparent Grade
Röhm ACRYLITE® MD™ H12 Acrylic Polymer For Medical Diagnostics
RTP Company PermaStat® 302 FR Polycarbonate (PC), ESD Protection - Permanently Anti-static - Glass Fiber - Flame Retardant
RTP Company PermaStat® 1800 A FR Polycarbonate/Acrylic Alloy (PC/PMMA), Flame Retardant - Permanently Anti-static - ESD Protection - UL94 V-0

PQZWA2174 / 91000

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.