MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyram PlusTek PB145 Nylon 6, Injection Molding
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Polyamide 6 for fast cycle injection molding

Information provided by Polyram Ram On Ind.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³DIN 53479
Water Absorption 9.5 %9.5 %DIN 53495
Moisture Absorption at Equilibrium 3.0 %3.0 %50%RH; DIN 53714
Linear Mold Shrinkage 0.012 - 0.016 cm/cm0.012 - 0.016 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM-D785
Tensile Strength, Yield 95.0 MPa13800 psiASTM-D638
Elongation at Break 20 %20 %ASTM-D638
Flexural Strength 110 MPa16000 psiASTM D790
Flexural Modulus 2.60 GPa377 ksiASTM-D790
Izod Impact, Notched 0.500 J/cm
@Temperature 23.0 °C
0.937 ft-lb/in
@Temperature 73.4 °F
ASTM-D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmDIN 53482
Surface Resistance 1.00e+13 ohm1.00e+13 ohmDIN 53482
Dielectric Constant 3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 100 kV/mm2540 kV/inVDE 0303/4
 
Thermal PropertiesMetricEnglishComments
Melting Point 218 °C424 °F
Maximum Service Temperature, Air 80.0 °C176 °FContinuous Use
 180 °C356 °FShort peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 185 °C365 °FDIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FDIN 53461
Flammability, UL94 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyram PlusTek PB140 Nylon 6, Injection Molding
Polyram PlusTek PB150 Nylon 6, Injection Molding
Sax Polymers SAXAMID 126 Nylon 6, Injection Molding Grade
Sax Polymers SAXAMID 126H Nylon 6, Injection Molding Grade
Sax Polymers SAXAMID 136Q32 Nylon 6, Injection Molding Grade

PPOLYRA169 / 57431

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.