Physical Properties | Metric | English | Comments |
---|
Density | 1.14 g/cc | 0.0412 lb/in³ |
Water Absorption | 1.6 % @Time 86400 sec | 1.6 % @Time 24.0 hour |
Moisture Absorption at Equilibrium | 2.4 % | 2.4 % |
Linear Mold Shrinkage, Flow | 0.013 cm/cm @Thickness 2.00 mm | 0.013 in/in @Thickness 0.0787 in |
Linear Mold Shrinkage, Transverse | 0.017 cm/cm @Thickness 2.00 mm | 0.017 in/in @Thickness 0.0787 in |
|
Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength at Break | 64.0 MPa | 9280 psi |
| 90.0 MPa | 13100 psi |
Tensile Strength, Yield | 67.0 MPa | 9720 psi |
| 95.0 MPa | 13800 psi |
Elongation at Break | 15 % | 15 % |
| 23 % | 23 % |
Elongation at Yield | 5.2 % | 5.2 % |
| 18 % | 18 % |
Tensile Modulus | 2.30 GPa | 334 ksi |
| 3.40 GPa | 493 ksi |
Flexural Strength | 28.0 MPa | 4060 psi |
| 103 MPa | 14900 psi |
Flexural Modulus | 1.20 GPa | 174 ksi |
| 3.30 GPa | 479 ksi |
Poissons Ratio | 0.40 | 0.40 |
Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -40.0 °C | 1.43 ft-lb/in² @Temperature -40.0 °F |
| 3.00 kJ/m² @Temperature -30.0 °C | 1.43 ft-lb/in² @Temperature -22.0 °F |
| 4.00 kJ/m² @Temperature -40.0 °C | 1.90 ft-lb/in² @Temperature -40.0 °F |
| 4.00 kJ/m² @Temperature -30.0 °C | 1.90 ft-lb/in² @Temperature -22.0 °F |
| 4.00 kJ/m² @Temperature 23.0 °C | 1.90 ft-lb/in² @Temperature 73.4 °F |
| 6.00 kJ/m² @Temperature 23.0 °C | 2.86 ft-lb/in² @Temperature 73.4 °F |
Charpy Impact Unnotched | NB @Temperature -40.0 °C | NB @Temperature -40.0 °F |
| NB @Temperature -40.0 °C | NB @Temperature -40.0 °F |
| NB @Temperature -30.0 °C | NB @Temperature -22.0 °F |
| NB @Temperature -30.0 °C | NB @Temperature -22.0 °F |
| NB @Temperature 23.0 °C | NB @Temperature 73.4 °F |
| NB @Temperature 23.0 °C | NB @Temperature 73.4 °F |
Charpy Impact, Notched | 0.300 J/cm² @Temperature -40.0 °C | 1.43 ft-lb/in² @Temperature -40.0 °F |
| 0.300 J/cm² @Temperature -40.0 °C | 1.43 ft-lb/in² @Temperature -40.0 °F |
| 0.300 J/cm² @Temperature -30.0 °C | 1.43 ft-lb/in² @Temperature -22.0 °F |
| 0.300 J/cm² @Temperature -30.0 °C | 1.43 ft-lb/in² @Temperature -22.0 °F |
| 0.400 J/cm² @Temperature 23.0 °C | 1.90 ft-lb/in² @Temperature 73.4 °F |
| 0.600 J/cm² @Temperature 23.0 °C | 2.86 ft-lb/in² @Temperature 73.4 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Arc Resistance | 120 - 180 sec @Thickness 3.00 mm | 120 - 180 sec @Thickness 0.118 in |
Comparative Tracking Index | 600 V @Thickness 3.00 mm | 600 V @Thickness 0.118 in |
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec |
| 15 - 30 sec | 15 - 30 sec |
| 30 - 60 sec | 30 - 60 sec |
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs |
| >= 120 arcs | >= 120 arcs |
| >= 120 arcs | >= 120 arcs |
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear, Parallel to Flow | 100 µm/m-°C @Thickness 2.00 mm, Temperature 35.0 - 55.0 °C | 55.6 µin/in-°F @Thickness 0.0787 in, Temperature 95.0 - 131 °F |
CTE, linear, Transverse to Flow | 100 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C | 55.6 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
Melting Point | 262 °C | 504 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F |
| 232 °C | 450 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F |
UL RTI, Electrical | 130 °C @Thickness 0.710 mm | 266 °F @Thickness 0.0280 in |
| 130 °C @Thickness 1.50 mm | 266 °F @Thickness 0.0591 in |
| 130 °C @Thickness 3.00 mm | 266 °F @Thickness 0.118 in |
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.710 mm | 167 °F @Thickness 0.0280 in |
| 75.0 °C @Thickness 1.50 mm | 167 °F @Thickness 0.0591 in |
| 75.0 °C @Thickness 3.00 mm | 167 °F @Thickness 0.118 in |
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 0.710 mm | 185 °F @Thickness 0.0280 in |
| 85.0 °C @Thickness 1.50 mm | 185 °F @Thickness 0.0591 in |
| 85.0 °C @Thickness 3.00 mm | 185 °F @Thickness 0.118 in |
Flammability, UL94 | V-2 @Thickness 0.710 mm | V-2 @Thickness 0.0280 in |
| V-2 @Thickness 1.50 mm | V-2 @Thickness 0.0591 in |
| V-2 @Thickness 3.00 mm | V-2 @Thickness 0.118 in |
Glow Wire Ignition Temperature | 850 °C @Thickness 0.710 mm | 1560 °F @Thickness 0.0280 in |
| 850 °C @Thickness 1.50 mm | 1560 °F @Thickness 0.0591 in |
| 850 °C @Thickness 3.00 mm | 1560 °F @Thickness 0.118 in |
Glow Wire Flammability Index | 960 °C @Thickness 0.710 mm | 1760 °F @Thickness 0.0280 in |
| 960 °C @Thickness 1.50 mm | 1760 °F @Thickness 0.0591 in |
| 960 °C @Thickness 3.00 mm | 1760 °F @Thickness 0.118 in |
|
Processing Properties | Metric | English | Comments |
---|
Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F |
Middle Barrel Temperature | 270 - 285 °C | 518 - 545 °F |
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F |
Nozzle Temperature | 280 - 300 °C | 536 - 572 °F |
Melt Temperature | 285 - 300 °C | 545 - 572 °F |
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F |
Drying Temperature | 80.0 °C | 176 °F |
Dry Time | 4.00 hour | 4.00 hour |
|
Descriptive Properties |
---|
Additive | Lubricant |
Agency Ratings | ASTM, D4066 PA0131 |
| ASTM, D6779 PA0131 |
| EC, 1935/2004 |
| EU, 10/2011 |
| EU, 2023/2006 |
| FDA, 21 CFR 177.1500 |
| FED, L-P-410A |
Appearance | Natural Color |
Features | Fast Molding Cycle |
| General Purpose |
| Good Mold Release |
| Good Stiffness |
| High Rigidity |
| Lubricated |
| Nucleated |
Forms | Pellets |
Outdoor Suitability | f2 |
Processing Method | Injection Molding |
Region | North America, Europe, Asia Pacific |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.