MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: Description: Ultramid® T 4381 LDS is a semi-crystalline, partially aromatic high temperature polyamide (PA6/6T) for laser direct structuring (LPKFLDS®). As the material is reinforced with 10% fiberglass and 25% mineral filling, high-strength mechatronic plastic parts can be manufactured efficiently, quickly and flexibly with LDS. The innovative material offers a broad processing window for optimal results regarding: laser activation, metallization, adhesion of the conductors. Ultramid T 4381 LDS is based on Ultramid T and offers an ideal combination of high melting temperature, good processability and low water absorption. This specialty from BASF’s engineering plastics is already being used in electrical engineering and automotive construction, especially where high heat distortion temperature is required.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.52 g/cc0.0549 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.80 - 1.2 %0.80 - 1.2 %50% RH; ISO 62
Viscosity Measurement 130130ISO 307
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 110 MPa16000 psi5mm/min; ISO 527-2
Tensile Strength, Yield 48.0 MPa6960 psiISO 527
Elongation at Break 2.1 %2.1 %ISO 527-2
Elongation at Yield 5.0 %5.0 %ISO 527
Tensile Modulus 9.00 GPa1310 ksiISO 527-2
Charpy Impact Unnotched 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+12 ohm-cm4.00e+12 ohm-cmIEC 60093
Surface Resistance >= 1.00e+16 ohm>= 1.00e+16 ohmISO 60093
Dielectric Constant 4.4
@Frequency 1e+6 Hz
4.4
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.015
@Frequency 1e+6 Hz
0.015
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C16.7 µin/in-°FDIN 53152
CTE, linear, Transverse to Flow 50.0 µm/m-°C27.8 µin/in-°FDIN 53752
Melting Point 295 °C563 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 265 °C509 °FISO 75-2
 
Descriptive Properties
ColorBlack
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Conditioned)
Kingfa LONOY 2100 LT PC/PET Alloy
Plastcom SLOVAMID® 6/6T GF 35 TS PA6/6T reinforced with glass fiber, improved heat resistance
EMS-Grivory Grivory® HT XE 4027 black 9916 PA*-GF30
Ensinger TECASINT™ 2021 Polyimide, Brown (PI)

PBASG0354 / 131987

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.