MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 9500B Double Coated Tapes with Adhesive 350
Categories: Polymer; Adhesive

Material Notes: 3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a medium-firm acrylic adhesive that provides a combination of high wet grab and initial adhesion and good shear holding power to a wide variety of materials, including many plastics.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 25.4 microns1.00 milCarrier
 58.4 microns2.30 milFaceside Adhesive
 58.4 microns2.30 milBackside Adhesive
 114 microns4.50 milCaliper
 142 microns5.60 milTotal Thickness
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.36156 kN/m2.0625 pliHDPE, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
 0.482 kN/m2.75 pliPolypropylene, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
 0.657 kN/m3.75 pliPolycarbonate, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
 0.77789 kN/m4.4375 pliStainless Steel, 90°, 15 min RT; ASTM D3330
 0.8108 kN/m4.625 pliABS, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
 0.84363 kN/m4.8125 pliPolyester, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
 1.0189 kN/m5.8125 pliStainless Steel, 90°, 72 hr RT; ASTM D3330
 1.3257 kN/m7.5625 pliStainless Steel, 90°, 72 hr at 70°C; ASTM D3330
 1.53 kN/m8.75 pliStainless Steel, 180°, 2 mil al foil, 72 hr RT; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °FLong term
 177 °C351 °FShort term
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
LinerPolycoated Kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 950 Adhesive Transfer Tapes with Adhesive 300

PMM33279 / 168026

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.