MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kotec Carbotex K-20UV Polycarbonate, General Purpose, UV Stability Grade
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, UV Stabilized

Material Notes: Features: UV Stability, High flow, Transparent
Applications: OA equipment, Communications, Precision parts, Machineries, Lighting Covers, Safety products, E & E parts, Household applications, Leisure articles

Information provided by Kotec Corporation

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Water Absorption 0.20 %
@Temperature 23.0 °C,
Time 86400 sec
0.20 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D995
Melt Flow 20 g/10 min
@Load 1.20 kg,
Temperature 300 °C
20 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120
Tensile Strength at Break 63.0 MPa9140 psiASTM D638
Elongation at Break 120 %120 %ASTM D638
Flexural Strength 85.0 MPa12300 psiASTM D790
Flexural Modulus 2.16 GPa313 ksiASTM D790
Izod Impact, Notched 7.40 J/cm
@Temperature 23.0 °C
13.9 ft-lb/in
@Temperature 73.4 °F
V-Notched 1/8"; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm508 kV/inASTM D149
Dissipation Factor 0.0090
@Frequency 1e+6 Hz
0.0090
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 110 sec110 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 131 °C268 °FASTM D648
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.581.58ASTM D542
Haze <= 1.0 %
@Thickness 3.00 mm
<= 1.0 %
@Thickness 0.118 in
ASTM D1003
Transmission, Visible 89 %
@Thickness 3.00 mm
89 %
@Thickness 0.118 in
ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUPOY GP1000MU PC, Transparent
Techmer ES HiFill FR® PC FR
LG Chemical LUPOY GP1000HU PC, Transparent
LG Chemical Lupoy 1302HP-07 Polycarbonate Resin
LG Chemical Lupoy 1302-05 Polycarbonate Resin

PKOTEC003 / 93233

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.