System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
NAECO® ELKON® 35S Silver Tungsten contact material ASTM B631, Class B, infiltrated
Categories:
Metal
;
Metal Matrix Composite
;
Nonferrous Metal
;
Precious Metal
;
Silver Alloy
;
Refractory Metal
;
Tungsten Alloy
Material Notes:
For arcing and current carrying electrical contacts; household and power circuit breakers.
Information provided by NAECO, LLC.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
14.77
g/cc
0.5336
lb/in³
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell B
78
78
Electrical Properties
Metric
English
Comments
Electrical Resistivity
0.00000313
ohm-cm
0.00000313
ohm-cm
(55% IACS)
Thermal Properties
Metric
English
Comments
Thermal Conductivity
170
W/m-K
1180
BTU-in/hr-ft²-°F
Melting Point
980
-
3410
°C
1800
-
6170
°F
Solidus
980
°C
1800
°F
Liquidus
3410
°C
6170
°F
Component Elements Properties
Metric
English
Comments
Silver, Ag
50 %
50 %
Tungsten, W
50 %
50 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
NAECO® ELKON® 3042 Silver Tungsten Carbide contact material ASTM B663
NAECO® ELKON® 1060 Silver Tungsten Carbide Contact Material
NAECO® NAECOMET® D154F Pre-Oxidized Silver Cadmium Oxide Contact Material ASTM B781 Table 3
NAECO® ELKON® 3150 Silver Tungsten Carbide contact material ASTM B663 Table 2, Class B
NAECO® ELKON® 2150 Silver Tungsten contact material ASTM B631, Class C, press-sinter-repress
NCMV841 / 192417
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.