MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ipiranga Petrochem PH 1310 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not produce catalyst residues (due to its high catalytic yield).

Raw materials are supplied by COPESUL. Following pre-treatment, they are sent, with the catalytic system, into two loop reactors and one gas-phase reactor. This plant produces PP homopolymer, random copolymer, heterophase copolymer and terpolymer.

The product leaves the reactors in the shape of spherical grains. The grains are sent to the extrusion site, where stabilizers are added to them. They are then turned into pellets by an extruding press. The pelletized material is first sent to mixing and storage silos. Later, this material is sent to the packaging area.

Applications:

  • caps with seals
  • household goods
  • furniture
  • lids
  • toys

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 11 - 15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
11 - 15 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 111111ASTM D785-98
Tensile Strength, Yield 369 MPa53500 psiASTM D638-02
Elongation at Yield 8.2 %8.2 %ASTM D638-02
Flexural Modulus, 1% Secant 1550 MPa225000 psiASTM D790-02
Izod Impact, Notched 0.350 J/cm0.656 ft-lb/inASTM D256-03
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FASTM D648-97
Vicat Softening Point 153 °C307 °FASTM D1525-97
 
Optical PropertiesMetricEnglishComments
Haze 90 %
@Thickness 1.60 mm
90 %
@Thickness 0.0630 in
ASTM D1003A-00

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® C3 GF 60 1 (4659) PA66/6 Dry, 60% Glass Filled
Polyram Polytron P60B11 Homopolymer Polypropylene, Chemically Coupled 60% LGF
Ensinger TECATEC CF60 Polyaryletherketone (PAEK) Laminate
Avient OnForce™ LFT UR-60 LGF/000 Natural Polyurethane, PUR
LyondellBasell Moplen EP400H Polypropylene, Impact Modified; Molded/Extruded

PIPIRA42 / 48375

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.