MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hifax TYC007P BLK Thermoplastic Olefinic Elastomer, mineral Filled
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Hifax polypropylene resins based on the Catalloy process are used in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable), and automotive industries. Hifax priovides good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion.

Hifax TYC007P BLK very high melt flow, very high flexural modulus, UV-stabilized, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of properties and processability. It is typically used for automotive bumper fascias. Applications: Automotive Parts, Bumpers, Exterior Automotive Applications

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183-1
Melt Flow 31 g/10 min
@Load 2.16 kg,
Temperature 230 °C
31 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 6363ISO 2039-2
Tensile Strength, Yield 20.0 MPa2900 psi50mm/min; ISO 527-1,-2
Tensile Modulus 2.00 GPa290 ksi50mm/mim, chord; ISO 527-1,-2
Flexural Modulus 2.10 GPa305 ksi2mm/min; ISO 178
Izod Impact, Notched  0.0500 J/cm
@Temperature -30.0 °C
0.0937 ft-lb/in
@Temperature -22.0 °F
ASTM D 256
 0.420 J/cm
@Temperature 23.0 °C
0.787 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C239 °Funannealed; ISO 75B-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 59.0 °C138 °Funannealed; ISO 75A-1,-2
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Daplen™ EE255AE Polypropylene TPO Compound
Borealis Daplen™ EE260AE Scratch Resistant Polypropylene Compound
Borealis Daplen™ EF210AE Polypropylene TPO Compound
Borealis Daplen™ EF209AE Polypropylene TPO Compound
Domo Technyl® A 246M Nylon 66, Impact Grade, EH0

PEQT7427 / 219064

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.