MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® B50L 01 PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Ultramid B50L 01 is a high-viscosity, lubricated, general-purpose extrusion PA6 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or legislations for other countries will be provided on request.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Water Absorption 9.5 %9.5 %ISO 62
Moisture Absorption at Equilibrium 2.6 %2.6 %23°C/50% R.H.; ISO 62
Relative Viscosity 5.0 cP5.0 cPISO Test; 96 % SAV
Viscosity Number 320 cm³/g3.20 dl/g
Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/inASTM Data; MD
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 275 °C
8.0 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 80.0 MPa11600 psi2 in/min; ASTM Test
 90.0 MPa13100 psi50mm/min; ISO 527
Elongation at Break >= 50 %>= 50 %50mm/min, Nominal strain; ISO 527
Elongation at Yield 4.5 %4.5 %50mm/min; ISO 527
Tensile Modulus 3.00 GPa435 ksi1mm/min; ISO 527
 3.00 GPa435 ksiASTM Test
Izod Impact, Notched 0.530 J/cm
@Temperature -40.0 °C
0.993 ft-lb/in
@Temperature -40.0 °F
ASTM Test
 1.34 J/cm
@Thickness 3.17 mm
2.51 ft-lb/in
@Thickness 0.125 in
ASTM Test
Charpy Impact Unnotched NBNBISO 179
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant  3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
IEC 60250
 4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.023
@Frequency 1e+6 Hz
0.023
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
22.2 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM Test
CTE, linear, Parallel to Flow 85.0 µm/m-°C47.2 µin/in-°FISO 11359
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FASTM Test
 160 °C320 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C129 °FASTM Test
 65.0 °C149 °FISO 75
Vicat Softening Point 204 °C399 °F(50 °C/h / 50N) - B/50; ISO 306
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21 CFR 177.1500
 
Descriptive Properties
ColorNatural
Commercial StatusNorth America and Europe
FormPellets
Impact ModifiedNo
Primary Processing TechniqueFilm Extrusion
ProcessingFilm Extrusion
 Profile Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B50 01 PA6
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Dry)
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Conditioned)
Domo TECHNYL® A 205F PA66, DRY
ExxonMobil Santoprene® 103-50 Thermoplastic Elastomer

PBASF9355 / 85119

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.