A fully hydrogenated butadiene acrylonitrile copolymer (less than 1% residual double bonds), which provides vulcanizate with superior resistance to heat, ozone and excellent resistance to non-polar hydrocarbon fluids including those containing aggressive additives. With this level of unsaturation, Therban 3607-based compounds can only be vulcanized with peroxides or high-energy radiation. The incorporation of a crosslinking co-agent is recommended for optimized physical properties of both unaged and aged vulcanizates.Information provided by Lanxess. |