MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem GM5240PR HDPE High Density Extrusion Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: GM5240PR is a high-density polyethylene compound specially developed for the manufacturing of pipes, underground conduits, and steel pipe coating. This resin is produced with bimodal technology and shows excellent mechanical properties and resistance to stress cracking. GM5240PR contains carbon black pigment that protects it against ultraviolet radiation action and photodegradation. Its applications include: triple-layer coating for metallic pipes, localized irrigation pipes, and ducts for mining.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.957 g/cc0.0346 lb/in³ASTM-D792
ESCR 100% Igepal® >= 1000 hour
@Thickness 2.00 mm,
Temperature 50.0 °C
>= 1000 hour
@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Melt Flow 0.55 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.55 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6161ASTM-D2240
Tensile Strength at Break 28.0 MPa4060 psiASTM-D638
Tensile Strength, Yield 23.0 MPa3340 psiASTM-D638
Elongation at Break 840 %840 %ASTM-D638
Elongation at Yield 9.9 %9.9 %ASTM-D638
Flexural Modulus, 1% Secant 980 MPa142000 psiASTM-D790
Izod Impact, Notched 0.850 J/cm1.59 ft-lb/inASTM-D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C154 °FASTM-D648
Vicat Softening Point 121 °C
@Load 1.02 kg
250 °F
@Load 2.25 lb
ASTM-D1525
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 2.4 %2.4 %Black Content; ASTM-D1603
 
Descriptive Properties
UV Absorption Coefficient (Abs/cm)> 3000ASTM-D3349

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 9346 HDPE Natural Pipe Resin
Braskem ES 002G HDPE Pipe Extrusion Polyethylene
Chevron Phillips HiD® 9348 HDPE Natural Pipe Resin
Braskem GF4950HS HDPE Blow Molding Polyethylene Copolymer
LyondellBasell Alathon® L5906 High Density Polyethylene

PBRAS801 / 106647

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.