MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

CMT Materials REN Shape® Express 2000 Tooling Board, Modeling Board, Adhesive Products  (discontinued **)
Categories: Polymer

Material Notes: CMT Materials offers the complete line of REN Shape tooling board, modeling board, and related adhesive products. Vacuum formers and thermoformers use these products as prototype and low volume production molds when forming in applications where metal molds do not makes sense due to time or cost considerations. CMT can help in selecting the proper board material for specific forming applications considering factors such as surface quality, ease in machining, tool durability, and forming temperature.

Information Provided by CMT Materials, Inc.

Key Words: Renshape
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.79 g/cc0.0648 lb/in³ASTM D-792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9191ASTM D-2240
Tensile Strength, Ultimate 62.1 MPa9000 psiASTM D-638
Flexural Strength 82.7 MPa12000 psiASTM D-790
Flexural Modulus 8.27 GPa1200 ksiASTM D-790
Compressive Strength 252 MPa36500 psiASTM D-695
Compressive Modulus 6.21 GPa900 ksiASTM D-695
 
Thermal PropertiesMetricEnglishComments
CTE, linear 37.8 µm/m-°C21.0 µin/in-°FASTM D-3386
Glass Transition Temp, Tg 258 °C496 °FASTM D-4065
 
Descriptive Properties
ColorGray

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CMT Materials REN Shape® 440 Tooling Board, Modeling Board, Adhesive Products
Wacker Silres® REN 80 Heat Resistant Silicone Coating
Wacker Silres® REN 60 Heat Resistant Silicone Coating
CMT Materials REN Shape® 550 Tooling Board, Modeling Board, Adhesive Products
CMT Materials REN Shape® 5025 Tooling Board, Modeling Board, Adhesive Products

PCMTZ004 / 93171

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.