MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BASF Ultramid® KR 4357 G6 30% Glass Filled PA6/6T (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties remain constant after moisture absorption up to a temperature of 60°C [140°F], for instance, for automotive plug-in connectors.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183
Moisture Absorption at Equilibrium >= 0.80 %>= 0.80 %50% RH; ISO 62
 >= 4.5 %>= 4.5 %Saturation; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  165 MPa
@Temperature 23.0 °C
23900 psi
@Temperature 73.4 °F
ISO 527
 249 MPa
@Temperature -40.0 °C
36100 psi
@Temperature -40.0 °F
ISO 527
Elongation at Break 3.5 %3.5 %ISO 527
Modulus of Elasticity 9.30 GPa1350 ksiISO 527-1/-2
Izod Impact, Notched (ISO) 23.0 kJ/m²
@Temperature 23.0 °C
10.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched  9.00 J/cm²
@Temperature -30.0 °C
42.8 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 9.50 J/cm²
@Temperature 23.0 °C
45.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 1.90 J/cm²
@Temperature 23.0 °C
9.04 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60093
Dielectric Constant 4.3
@Frequency 1e+6 Hz
4.3
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
13.9 µin/in-°F
@Temperature 73.4 - 176 °F
DIN 11359-1/-2
CTE, linear, Transverse to Flow 55.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
30.6 µin/in-°F
@Temperature 73.4 - 176 °F
DIN 11359-1/-2
Specific Heat Capacity 1.40 J/g-°C0.335 BTU/lb-°F
Melting Point 295 °C563 °FDIN 53765
Deflection Temperature at 1.8 MPa (264 psi) 270 °C518 °FISO 75-1/-2
Decomposition Temperature >= 350 °C>= 662 °F
UL RTI, Electrical 140 °C
@Thickness 1.50 mm
284 °F
@Thickness 0.0591 in
746B
UL RTI, Mechanical with Impact 110 °C
@Thickness 1.50 mm
230 °F
@Thickness 0.0591 in
746B
UL RTI, Mechanical without Impact 140 °C
@Thickness 1.50 mm
284 °F
@Thickness 0.0591 in
746B
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FHopper Throat
Zone 1 300 °C572 °FFeed Zone
Zone 2 310 °C590 °FCompression
Zone 3 320 °C608 °FMetering-zone
Zone 4 320 °C608 °FNozzle
 
Descriptive Properties
ColorBK 00564
Commercial StatusNorth America
Peripheral Screw Speed<0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Conditioned)
Evonik VESTAMID® HTplus M1634 PA6T/X, GF30
BASF Ultramid® C33 01 PA66/6 (Dry)
Nylene® 826 Nylon Copolymer
Overview of materials for Nylon 66, 30% Glass Fiber Filled

PBASG0296 / 131929

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.