MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem H 606 Thermoforming Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Description: H 606 is low melt flow rate homopolymer with general purpose additive package. This resin is designed for extrusion and thermoforming. H 606 presents excellent processability and high output, excellent stiffness/impact strength balance, high melt strength and low odor/taste transfer.

Applications: Thermoformed packaging for food, cosmetic, health care and cleaning products; Flat and corrugated sheets.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D792A
Melt Flow 2.1 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.1 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7575ASTM D785
Tensile Strength, Yield 35.0 MPa5080 psiASTM D638
Elongation at Yield 12 %12 %ASTM D638
Flexural Modulus 1.59 GPa231 ksiASTM D790
Izod Impact, Notched 0.380 J/cm
@Temperature 23.0 °C
0.712 ft-lb/in
@Temperature 73.4 °F
ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C196 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C133 °FASTM D648
Vicat Softening Point 153 °C307 °F-1kg; ASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsui ADMER® QF551A PP Type Polyolefin
LyondellBasell Moplen HP748H Polypropylene, Sheet/Thermoforming Grade
Braskem Prisma 6810 Thermoforming Polypropylene
Braskem HP 502H Extrusion Thermoforming Extrusion Blow Molding Polypropylene
Braskem H105-03NA Sheet Extrusion Thermoforming Polypropylene

PBRAS047 / 27781

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.