MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Crucible Steel CPM® Rex® 76®(HS), AISI M48 High Speed Steel Rex® 76®(HS)
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Tool Steel

Material Notes: CPM Rex 76 is a super high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It is heat treatable to HRC 68-70. Its high carbon, vanadium and cobalt contents provide abrasion resistance comparable to that of T15 and red hardness superior to that of M42. With its high hardness, fine grain size and uniform carbide distribution, CPM Rex 76 is an outstanding choice for special purpose cutting tools requiring high red hardness, high abrasion resistance, and good toughness.

The CPM process results in a homogeneous microstructure with a finer, more uniform carbide distribution imparting superior dimensional stability, grindability and toughness when compared to steels produced by conventional processes. The CPM process also allows the design of more highly alloyed grades which cannot be produced by conventional steelmaking.

Information provided by Crucible Specialty Metals.

Key Words: AISI M48 High Speed Steel
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.255 g/cc0.2982 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 285 - 311285 - 311Annealed
Hardness, Rockwell C 6767Hardening Temperature- 1165°C; Tempering Temperature- 565°C
 7070Hardening Temperature- 1200°C; Tempering Temperature- 525°C
Modulus of Elasticity 214 GPa31000 ksi
Flexural Strength 2296 MPa333000 psiHardening Temperature- 1200°C, Tempering Temperature- 525°C
 4365 MPa633100 psiHardening Temperature- 1165°C, Tempering Temperature- 565°C
Charpy Impact 8.00 J5.90 ft-lbHardening Temperature- 1200°C; Tempering Temperature- 525°C
 20.0 J14.8 ft-lbHardening Temperature- 1165°C; Tempering Temperature- 565°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.66 µm/m-°C
@Temperature 20.0 - 95.0 °C
5.922 µin/in-°F
@Temperature 68.0 - 203 °F
 10.8 µm/m-°C
@Temperature 20.0 - 200 °C
6.00 µin/in-°F
@Temperature 68.0 - 392 °F
 11.74 µm/m-°C
@Temperature 20.0 - 540 °C
6.522 µin/in-°F
@Temperature 68.0 - 1000 °F
Shrinkage -0.220 %
@Treatment Temp. 1190 °C
-0.220 %
@Treatment Temp. 2170 °F
Hardening
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.5 %1.5 %
Chromium, Cr 3.75 %3.75 %
Cobalt, Co 8.5 %8.5 %
Iron, Fe 67.93 %67.93 %As Remainder
Molybdenum, Mo 5.25 %5.25 %
Sulfur, S 0.070 - 0.22 %0.070 - 0.22 %
Tungsten, W 9.75 %9.75 %
Vanadium, V 3.1 %3.1 %
 
Descriptive Properties
Grindability; Metal Removed/Wheel Worn3.8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Latrobe Dynavan™ ASTM T15 Super High Speed Steel
Latrobe DuraTech™ M48 Powder Metal High Speed Steel (ASTM M48)
Bohler-Uddeholm BÖHLER S401(M1) High Speed Steel
Crucible Steel CPM® Rex® 45® (HS) High Speed Steel
Crucible Steel CPM® Rex® T15(HS), AISI T15 High Speed Steel Rex® T15(HS)

NCRUC011 / 16004

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.