MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman XIR 70 Film
Categories: Polymer; Film

Material Notes: XIR automotive film is transparent coated film that is encapsulated between layers of Saflex® PVB in laminated automotive glass to form a protective barrier against the harmful effects of the sun. The spectrally-selective metallic coating reflects heat-causing infrared (IR) rays without impairing visible light transmission. XIR laminated glass reduces solar heat gain an average of 35% more effectively than tinted glass.

Applications: Windscreen, Side Window, Sunroof, Back Glass, Quarter Glass

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesMetricEnglishComments
Transmission, Visible <= 54 %<= 54 %Total Solar; ISO 13837
 >= 71 %>= 71 %ASTM E308
 
Descriptive Properties
Reflectance<9.5%Visible, ISO 9050
 -2.0 to 2.0Color Rb, ASTM E308
 -4.7 to -0.7Color Ra, ASTM E308

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman XIR 70.48 Film
Eastman XIR 7241 Clear 6mm
Eastman Saflex® SG41 Interlayer
Eastman Saflex® RB11 Clear PVB interlayer
Eastman Saflex® DG41 Structural PVB interlayer

PEATM5677 / 222871

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.