POWERSIL® 555 R Dispersion Coating is a one component liquid silicone RTV system that is designed as an insulator coating for high voltage applications. When exposed to moisture in the air, POWERSIL® 555 R cures to a flexible elastomer with excellent electrical and mechanical properties. Special features: - Excellent unprimed adhesion
- Excellent unprimed adhesion
- One component, ready-to-use
- Easy to apply
- Sprayable or paintable
Application: Protective coating for glass, porcelain or epoxy insulators and other high-voltage insulations, where contamination causes service problems. POWERSIL® 555 R prevents the formation of wet conductive films and therefore the risk of tracking and especially flashovers.Information provided by Wacker Chemie AG. |