MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and puncture. Easier processing and excellent properties lead to significant high pressure LDPE replacement in many applications, yet with superior drawdown and enhanced toughness. Enable 23-05 resins are available with and without antiblock

Availability: Latin America, North America and South America

Additive:

  • Antiblock: 2000 ppm
  • Slip: No
  • Processing Aid: Yes
  • Thermal Stabilizer: Yes
Applications:
  • Agricultural Film
  • Blown Film
  • Collation Shrink
  • Food packaging
  • Form Fill and Seal Packaging
  • Heavy Duty Bags
  • Lamination Film
  • Multilayer Packaging Film
  • Shrink Film
  • Stand Up Pouches

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.927 g/cc0.0335 lb/in³ExxonMobil method
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 13.1 MPa1900 psiASTM D882
Film Tensile Strength at Yield, TD 15.2 MPa2200 psiASTM D882
Film Elongation at Break, MD 480 %480 %ASTM D882
Film Elongation at Break, TD 750 %750 %ASTM D882
Puncture Energy 2.94 J2.17 ft-lbExxonMobil Method
Elmendorf Tear Strength MD 40 g40 gASTM D1922
Elmendorf Tear Strength TD 670 g670 gASTM D1922
Dart Drop Test 140 g0.309 lbASTM D1709A
Film Tensile Strength at Break, MD 64.1 MPa9300 psiASTM D882
Film Tensile Strength at Break, TD 52.4 MPa7600 psiASTM D882
1% Secant Modulus, MD 310 MPa45000 psiASTM D882
1% Secant Modulus, TD 386 MPa56000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 119 °C<= 246 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesMetricEnglishComments
Haze 12 %12 %ASTM D1003
Gloss 42 %42 %45°; ASTM D2457
 
Descriptive Properties
Puncture Force11 lbfExxonMobil Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Enable™ 20-10HE Metallocene Polyethylene Resin
ExxonMobil Enable™ 23-05HH Metallocene Polyethylene Resin
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin
ExxonMobil Enable™ 20-05CB Metallocene Polyethylene Resin

PEX99009 / 175246

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.