MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Colorite Polymers Flexchem 6551-02 Vinyl Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Material Notes: Description: The Flexchem "51" series is a group of translucent, flexible, non-toxic vinyl compounds which were specifically developed to replace silicone in various applications. These compounds utilize a non-phthalate plasticizer system for use in medical device applications. This unique product line offers excellent release characteristics, rubber-like compression properties, good burst strength and durability. These compounds can even be solvent bonded for ease of assembly. Flexchem compounds can be extruded or injection molded; they do not require any special equipment for processing. A replacement for silicone in a nearly endless list of uses, including tubing for pumping applications, urinary drain sets, beverage spouts, gaskets, etc., Flexchem is available in durometers ranging from 35 to 65 shore A hardness. It is formulated utilizing only FDA sanctioned raw materials and has been designed for use in USP Class VI applications. For medical use, complete traceability and lot identification of all components in the Flexchem products are maintained at Colorite.

Information provided by Colorite Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565
Tensile Strength, Ultimate 15.4 MPa2240 psi
Elongation at Break 360 %360 %
100% Modulus 5.71 MPa
@Strain 100 %
828 psi
@Strain 100 %
Compression Set 43 %43 %RT for 22 hours
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Colorite Polymers 7066 Non-Phthalate 66 Series Vinyl Compound
Colorite Polymers 7077 Non-Phthalate 77 Series Vinyl Compound
Colorite Polymers Flexchem 3551-02 Vinyl Compound
Colorite Polymers Flexchem 5551-02 Vinyl Compound
Colorite Polymers 9511G-015 (Extrustion), 9512G-015 (Molding) Radiation Sterilizable Vinyl Compound

PCOL006 / 28725

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.