MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 2199 X 117875 A Polyetherimide (PEI), Carbon Nanotube - Static Dissipative - ESD Protection - High Purity
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 g/cc1.29 g/ccASTM D 792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
@Thickness 3.17 mm
0.0050 - 0.0070 in/in
@Thickness 0.125 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 96.5 MPa14000 psiASTM D 638
Elongation at Break 4.0 %4.0 %ASTM D 638
Tensile Modulus 3.45 GPa500 ksiASTM D 638
Flexural Strength 145 MPa21000 psiASTM D 790
Flexural Modulus 4.00 GPa580 ksiASTM D 790
Izod Impact, Notched 0.427 J/cm
@Thickness 3.17 mm
0.800 ft-lb/in
@Thickness 0.125 in
ASTM D 256
Izod Impact, Unnotched 3.20 J/cm
@Thickness 3.17 mm
6.00 ft-lb/in
@Thickness 0.125 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 10000 ohm-cm<= 10000 ohm-cmASTM D 257
Surface Resistance 1e+05 - 1.00e+8 ohm1e+05 - 1.00e+8 ohmESD STM11.11
Surface Resistivity per Square 1.00e+6 - 1.00e+9 ohm1.00e+6 - 1.00e+9 ohmASTM D 257
Static Decay <= 2.0 sec<= 2.0 secFTMS101C; 4046.1
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 199 °C390 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 354 - 399 °C670 - 750 °F
Mold Temperature 135 - 177 °C275 - 350 °F
Drying Temperature 149 °C
@Time 14400 sec
300 °F
@Time 4.00 hour
Moisture Content 0.040 %0.040 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 82.7 - 124 MPa12000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ovation Polymers OpteSTAT™ MB PC 1000 Polycarbonate-based Carbon Nanotube Compound
Nanocyl PLASTICYL™ PBT1501 Polybutylene Terephthalate - Carbon Nanotube Masterbatch
Ensinger Tecapeek® XP-115 Compression Molded PEEK Compound, Static Dissipative
Westlake Plastics Propylux® SD-X7 Polypropylene (static dissipative)
RTP Company RTP 3399 X 117884 F Polyvinylidene Fluoride (PVDF), Carbon Nanotube - ESD Protection - Static Dissipative

PQZTA11547 / 159169

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.