MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Avient Maxxam™ SY 89-22-7 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Maxxam ™ SY 89-22-7 is a polypropylene copolymer compound with a pre-dispersed blowing agent for up to 60% expansion. The compound offers consistent cell structure, dielectric properties, and strength on insulation walls as thin as 10 mils.

NOTE: 1. Typical properties of molded slab (0.075); Not to be construedas specifications.2. Foam density reduction depends upon loading level, temperatureand residence time before cooling.3. Recommended process temperature: 190°C to 220°C (375°F to430°F).

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.519 g/cc0.519 g/ccASTM D792
Melt Flow 2.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.1 g/10 min
@Load 4.76 lb,
Temperature 374 °F
Procedure A; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 23.4 MPa3390 psiType IV, 510 mm/min; ASTM D638
Elongation at Break 400 %400 %Type IV, 510 mm/min; ASTM D638
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.24
@Frequency 1000 Hz
2.24
@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.00030
@Frequency 1000 Hz
0.00030
@Frequency 1000 Hz
ASTM D150
 
Descriptive Properties
FeaturesFoamable
FormsPellets
Generic MaterialPP, Unspecified
Generic NamePolypropylene, Unspecified (PP, Unspecified)
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesCable Jacketing
 Communication Wire Insulation
 Wire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Pro-fax EP315J Polypropylene Copolymer
CENTROPLAST CENTROLAB HT Polypropylene Higher Temperatures
Avient Maxxam™ SY 89-23-7 Polypropylene
Avient Maxxam™ SY 89-21-1 Polypropylene

PH0POL0835 / 145404

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.