MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

GEHR Plastics PMMA Acrylic
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Polymethylmethacrylate is refractory and shows a good mechanical strength, tensile strength and hardness. PMMA is also scratch resistant and easy to polish. It shows good temperature resistance and UV-stability. The operating temperature of PMMA ranges from -40°C to approximately 70°C.

Properties:

  • very high mechanical strength and hardness
  • high mechanical rigidity
  • excellent transparency
  • easy to polish
  • good thermal stability
  • good insulation properties
  • low water absorption
  • excellent weather resistance
  • possible stress problems
  • low chemical resistance
  • brittle
Applications:
  • Display
  • Advertisement
  • food industry
  • conduit pipe for milk
  • tubes for lamps
  • hand rails
  • automotive parts

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccISO 1183
Moisture Absorption at Equilibrium 0.40 %0.40 %ISO 62
Water Absorption at Saturation 2.1 %2.1 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090ISO 868
Tensile Strength, Yield 72.0 MPa10400 psiISO 527
Elongation at Break 8.0 %8.0 %ISO 527
Modulus of Elasticity 3.215 GPa466.3 ksiISO 527
Charpy Impact Unnotched 2.00 J/cm²9.52 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+13 ohm-cm3.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmIEC 60093
Dielectric Constant 2.8
@Frequency 1e+6 Hz
2.8
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 30.0 kV/mm762 kV/inIEC 60243-1
Dielectric Loss Index 0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FISO 11359
Thermal Conductivity 0.190 W/m-K
@Temperature 20.0 °C
1.32 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
ISO 22007-4
Melting Point 106 °C223 °FDIN EN ISO 3146
Maximum Service Temperature, Air 70.0 °C158 °FUL 746B
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FISO 75
Vicat Softening Point 103 °C217 °FVST/B/50; ISO 306
Glass Transition Temp, Tg 106 °C223 °FDIN EN ISO 3146
Flammability, UL94 HBHBtest results without UL registration; UL 94
Oxygen Index 17 %17 %ASTM D2863
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %"transparent" but not quantified
 
Compliance PropertiesMetricEnglishComments
FDA YesYesPhysiological indifference
 
Descriptive Properties
Acid Resistanceyes
Aromatic Resistanceno
Bondabilityyes
CKW Resistancelimited
Colortransparent
Hydrocarbonate Resistanceyes
Hydroxide Resistanceyes
Ketone Resistancelimited
Physiological indifferenceyes, EEC
Resistance Against Hot Waterlimited
UV Stabilizationyes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Extruded
Isoflon PMMA Polymethyl-methacrylate
Overview of materials for Polycarbonate, Molded
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Gypsum (CaSO4 - 2H2O)

PGEHR011 / 79848

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.