MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Styrolux® 693D SBC
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styrolux® 693D is a clear styrene-butadiene copolymer (SBC) with a well balanced combination of toughness and clarity. Styrolux 693D is mainly used for thermoformed articles, especially in blends with general-purpose polystyrene. Styrolux® 693D contains a microcrystalline wax which acts as an antiblock providing processing benefits but decreases the printability. Good clarity, Very high toughness, Enhanced GPPS blend capability. Applications: Food and non-food packaging, Blown film, Cups for cold beverages, Thermoformed transparent containers, Lids & Boxes

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Key Words: 693 D
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ISO 1183
Water Absorption at Saturation 0.070 %
@Temperature 23.0 °C
0.070 %
@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage 0.0030 - 0.010 cm/cm0.0030 - 0.010 in/inISO 294-4
Melt Flow 12.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
12.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6464ISO 868
Tensile Strength, Yield 22.0 MPa3190 psiISO 527
Elongation at Break 260 %260 %Nominal; ISO 527
 260 %260 %ISO 527
Elongation at Yield 2.2 %2.2 %ISO 527
Tensile Modulus 1.30 GPa189 ksiISO 527
Flexural Strength 32.0 MPa4640 psiISO 178
Flexural Yield Strength 32.0 MPa
@Strain 5.0 %
4640 psi
@Strain 5.0 %
Flexural Modulus 1.40 GPa203 ksiISO 178
Izod Impact, Notched 0.350 J/cm0.656 ft-lb/inASTM D256
Izod Impact, Notched (ISO)  2.50 kJ/m²
@Temperature -30.0 °C
1.19 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 3.50 kJ/m²
@Temperature 23.0 °C
1.67 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant 2.52.5IEC 60250
Dissipation Factor  0.00030
@Frequency 100 Hz
0.00030
@Frequency 100 Hz
IEC 60250
 0.00080
@Frequency 1e+6 Hz
0.00080
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 - 90.0 µm/m-°C33.3 - 50.0 µin/in-°FISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C162 °Fannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 59.0 °C138 °Fannealed 4 hours at 80°C; ISO 75
Vicat Softening Point  48.0 °C
@Load 5.10 kg
118 °F
@Load 11.2 lb
VST/B/50. 50C/h; ISO 306
 76.0 °C
@Load 1.02 kg
169 °F
@Load 2.25 lb
VST/A/50. 50C/h; ISO 306
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.571.57Sodium D Line; ISO 489
Haze 2.0 %2.0 %ASTM 1003
Transmission, Visible 89 %
@Wavelength 550 nm
89 %
@Wavelength 550 nm
ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 250 °C356 - 482 °FISO 294
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °FISO 294
 
Descriptive Properties
ColorCrystal Clear
Commercial StatusEurope
Primary Processing TechniqueInjection Molding, Extrusion, and Blow Molding
Transparency0.89d=2mm, DIN 5036-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Kibiton® PB-5903 SBC
INEOS Styrolution Styrolux® GH 58 SBC
Chi Mei Kibiton® PB-5502 Styrene-Butadiene Copolymer
Chi Mei Kibiton® PB-5925 SBC
Chi Mei Kibiton® PB-5910 SBC

PBASG0640 / 132273

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.