MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® Redux® 610W (0.09 psf) Flame retarded epoxy film adhesive
Categories: Polymer; Adhesive; Film; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Redux 610 is a modified, flame-retarded epoxy film adhesive curing at 250°F. It is suitable for bonding metal to metal and for sandwich structures where flame retardancy and low heat release are required. Redux 610 is a hot melt film which is free from solvents and consequently has a very low volatile content.

Features: Cures in 1 hour at 250°F; Good lap-shear performance up to 212°F; Good peel performance in sandwich structures up to 175°F; Meets the heat release requirements of IMO test MSC 61 (67); Good tack, drape and handleability; Very low volatile content and low out gassing properties; Available unsupported or with a very lightweight glass carrier.
Applications: Metal to metal bonding; Sandwich constructions; Flame retarded performance

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Storage Temperature -17.8 °C0.000 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month
@Temperature -17.8 °C
18.0 Month
@Temperature 0.000 °F
 
Descriptive Properties
Areal Weight (psf)0.09
Roll Width (in)49
Standard Roll (ft2)1075
SupportWoven Glass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexWeb® HRH-10/F35 - 2.5 Nonmetallic Flex-Core Honeycomb
Hexcel® Redux® 641K Modified epoxy film adhesive for bonding metallic and composite components
Hexcel® HexWeb® HRH-10 - 1/4 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb
Hexcel® HexWeb® CR-PAA™ 1/8-5052-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb
Hexcel® HexWeb® CR III 3/8-5056-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb

PHEXC472 / 99291

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.