MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NOVA Chemicals Novapol® LC-0717-A LDPE Extrusion Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: High speeds, Low coating weights, Excellent adhesion, Excellent drawdown, Excellent sealability

Applications: Sugar pouch stock; Popsicle wrap, Multi-wall bags, High speed/low coating weight paper coating, Flexible and snack food packaging, Coating of non-porous substrates

Additives: Base resin

Information provided by NOVA Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 g/cc0.0331 lb/in³ASTM D792
Water Vapor Transmission 18.0 g/m²/day
@Temperature 37.8 °C
1.16 g/100 in²/day
@Temperature 100 °F
90% RH; 30 lb Kraft paper samples with LDPE coating weight of 15 lb/ream; ASTM E96
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Neck In 5.50 cm2.17 inat 1000 ft/min; Neck-in reported is the total of both sides; NOVA Chemicals test method
Drawdown >= 9.10 m/s>= 1790 ft/minNOVA Chemical test method
Coating Weight >= 6.40 g/m²>= 4.00 lb/reamTAPPI test method; ASTM D539
 
Mechanical PropertiesMetricEnglishComments
Hot Tack Strength 225 g/25 mm225 g/inTests done on samples with a coating weight of 12 lb/ream, prepared under the following extrusion coating conditions: Output Rate: 3 lb/hr/in, Melt Temp: 600°F, Die Width: 12 in, Substrate: 40 lb Kraft paper. Mfr reports 450 g per 50 mm (2 in).
Heat Seal Strength 1400 g/25 mm3.09 lb/inTests done on samples with a coating weight of 12 lb/ream, prepared under the following extrusion coating conditions: Output Rate: 3 lb/hr/in, Melt Temp: 600°F, Die Width: 12 in, Substrate: 40 lb Kraft paper; ASTM D517
 
Processing PropertiesMetricEnglishComments
Melt Temperature 315 - 325 °C599 - 617 °FUntreated substrate. Optimum adhesion is obtained at a draw span of about 10 cm.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals Novapol® LC-0517-A LDPE Extrusion Resin
NOVA Chemicals Novapol® LC-0522-A LDPE Extrusion Resin
Braskem BI 818 LDPE Injection Molding Polyethylene
Chevron Phillips 4538B LDPE Injection Molding Resin
Chevron Phillips KN 230B LDPE Injection Molding Resin

PNOVA130 / 55031

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.