MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Borclear™ RE718CF Propylene Alpha Olefin Copolymer for Metallizable Cast Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Borclear RE718CF is a propylene alpha olefin copolymer resin formulation with antiblocking agent and without Ca-stearate, especially developed for the manufacturing of unoriented cast films for metallizing. It is specifically designed to be coextruded as a skin layer in combination with a high crystalline homopolymer core layer of Bormod HD915CF

Borclear RE718CF is suitable for various high quality film applications including metallisable cast film (metallized layer and heat seal layer)

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 - 0.910 g/cc0.0325 - 0.0329 lb/in³ISO 1183
Thickness 50.0 microns1.97 mil
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 650 %650 %ISO 527-3
Film Elongation at Break, TD 850 %850 %ISO 527-3
Flexural Modulus 0.950 GPa138 ksiISO 178
Secant Modulus, MD 0.400 GPa58.0 ksiISO 527-3
Secant Modulus, TD 0.500 GPa72.5 ksiISO 527-3
Impact 59.559.5Damaging Force (N); ISO 7765-2
Impact Test 1.40 J1.03 ft-lbPenetration Energy; ISO 7765-3
Film Tensile Strength at Break, MD 45.0 - 55.0 MPa6530 - 7980 psiISO 527-3
Film Tensile Strength at Break, TD 35.0 - 55.0 MPa5080 - 7980 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 138 - 144 °C280 - 291 °FISO 3146
Vicat Softening Point 130 °C266 °FISO 306
 
Optical PropertiesMetricEnglishComments
Haze <= 1.5 %<= 1.5 %ASTM D1003
Gloss >= 130 %>= 130 %At 20°C; ASTM D2457
Transmission, Visible 90 %90 %clear; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Borclear™ RD738CF Propylene Alpha Olefin Copolymer for Cast Film
Overview of materials for Polypropylene, Film Grade
Borealis RB707CF Polypropylene Random Copolymer for Blown Film

PBOREA041 / 27348

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.