MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Parker Chomerics THERMFLOW T725 Non-Silicone, Phase-Change Thermal Interface Pad
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: THERMFLOW® phase-change Thermal Interface Materials (TIM) are designed to minimize the thermal resistance between power dissipating electronic components and heat sinks. This low thermal resistance path maximizes heat sink performance and improved component reliability. At room temperature, THERMFLOW® materials are solid and easy to handle. This allows them to be consistently and cleanly applied as dry pads to a heat sink or component surface. THERMFLOW® material softens as it reaches component operation temperatures. With light clamping pressure it will readily conform to both mating surfaces. This ability to completely fill interfacial air gaps and voids typical of component packages and heat sinks allows THERMFLOW® pads to achieve performance superior to any other thermal interface materials. THERMFLOW® products are electrically non-conductive. However, since metal-to-metal contact is possible after the material undergoes phase-change in a typical heat sink assembly. In general, THERMFLOW® pads should not be used as electrical insulators –PC07DM-7 is offered as a dielectric version.

Typical Applications: Microprocessors, Graphics Processors, Chipsets, Memory Modules, Power Modules, Power Semiconductors.

Product Attributes: Excellent thermal performance; Inherently tack-no adhesive required; Ideal for vertical applications; Sticky nature limits flowing in vertical applications and Tabs available for easy removal

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D792
Thickness 127 microns5.00 mil
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.700 W/m-K4.86 BTU-in/hr-ft²-°F@ 50 psi; ASTM D5470
 0.254 W/m-K
@Pressure 0.0690 MPa
1.76 BTU-in/hr-ft²-°F
@Pressure 10.0 psi
ASTM D5470
 0.463 W/m-K
@Pressure 0.172 MPa
3.21 BTU-in/hr-ft²-°F
@Pressure 24.9 psi
ASTM D5470
 0.693 W/m-K
@Pressure 0.345 MPa
4.81 BTU-in/hr-ft²-°F
@Pressure 50.0 psi
ASTM D5470
Melting Point 58.0 °C136 °FASTM D3418
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 MonthFrom date of shipment; Chomerics
 
Descriptive Properties
CarrierNone
ColorPink
Phase Transition Temperature55°CASTM D3418
Weight Loss<0.5%125°C for 48 Hours

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aptek THERM-PAD 1100 Thermally conductive silicone pad
Indium Corp. Indalloy® 19 In-Bi-Sn Fusible Alloy
Parker Chomerics THERMFLOW® T710 with PSA Non-Silicone, Phase-Change Thermal Interface Pad
Parker Chomerics THERMFLOW® T777 Non-Silicone, Phase-Change Thermal Interface Pad
Parker Chomerics THERMFLOW® T558 Non-Silicone, Phase-Change Thermal Interface Pad

PCHOME009 / 28231

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.