MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Oxford Polymers PC/ABS 604i-FR PC/ABS, Flame retardant
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: Product Description: Amorphous, Polycarbonate & ABS, Flame retardant, Injection Molding Grade, VO rated @ 3.0mm. V2 rated @ 1.5mm

Processing and Delivery Form: Pellets and Injection Molding

Additives: Impact modifiers, Flame retardants

Special Characteristics: VO rated to 3.0mm, V2 rated to 1.5mm.and Available in all colors

Information provided by Oxford Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ASTM D792
Water Absorption at Saturation 0.35 %0.35 %ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.17 mm
0.0050 - 0.0070 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 56.5 MPa8200 psiASTM D638
Elongation at Break 50 %50 %ASTM D638
Flexural Strength 82.7 MPa12000 psiASTM D790
Flexural Modulus 2.93 GPa425 ksiASTM D790
Izod Impact, Notched 5.34 J/cm
@Thickness 3.17 mm
10.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C200 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 249 - 288 °C480 - 550 °F
Middle Barrel Temperature 254 - 293 °C490 - 560 °F
Front Barrel Temperature 260 - 302 °C500 - 575 °F
Nozzle Temperature 274 - 302 °C525 - 575 °F
Melt Temperature 274 - 302 °C525 - 575 °F
Mold Temperature 76.7 - 98.9 °C170 - 210 °F
Drying Temperature 93.3 - 110 °C200 - 230 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 2503 Polycarbonate/ABS Alloy (PC/ABS), Glass Fiber
LG Chemical LUPOY GP5006AF PC/ABS, Flame Retardant
LG Chemical LUPOY GP5008BFH PC/ABS, Flame Retardance
Oxford Polymers PC 1518 Unfilled Polycarbonate for Injection Molding
Oxford Polymers PC 68 Unfilled Polycarbonate for Injection and Extrusion Molding

POXF011 / 178441

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.